Textile fabric with high comfort
A technology for textile fabrics and comfort, applied in the field of high-comfort textile fabrics, can solve the problems of weak textile fabrics, uncomfortable wearing, and reduced comfort, so as to enhance wearing comfort and service life, and improve comfort. and softness, the effect of increasing the speed of drying
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] S1, the preparation of outer layer fabric: first select 8 parts of polyester fibers, 10 parts of spandex fibers and 12 parts of acrylic fibers respectively, then carry out scouring, bleaching and mercerizing pretreatment in sequence with the selected polyester fibers, spandex fibers and acrylic fibers, Then dye the polyester fiber, spandex fiber and acrylic fiber after the pretreatment, then clean the dyed fiber, and then place it in a dryer for drying. The drying temperature is 80°C, and the drying time is set to 1.5 hours, so that the moisture content in the fiber is less than 4%, and then the dried fiber is spun through a spinning machine to obtain polyester fiber, spandex fiber and acrylic fiber of the desired color, and then the polyester fiber, Spandex fiber and acrylic fiber are spun through a blending machine to obtain the outer fabric;
[0033] S2. Preparation of the inner layer fabric: first select 40 parts of cotton fibers, 70 parts of nanofibers, 30 parts of...
Embodiment 2
[0038] S1, the preparation of outer layer fabric: first select 5 parts of polyester fibers, 5 parts of spandex fibers and 10 parts of acrylic fibers respectively, then carry out scouring, bleaching and mercerizing pretreatment in sequence with the selected polyester fibers, spandex fibers and acrylic fibers, Then dye the polyester fibers, spandex fibers and acrylic fibers after the pretreatment, then clean the dyed fibers, and then place them in a dryer for drying. The drying temperature is 75°C, and the drying time is set to 1 hour, so that the moisture content in the fiber is less than 3%, and then the dried fiber is spun through a spinning machine to obtain polyester fiber, spandex fiber and acrylic fiber of the desired color, and then the polyester fiber, Spandex fiber and acrylic fiber are spun through a blending machine to obtain the outer fabric;
[0039] S2. Preparation of the inner layer fabric: first select 30 parts of cotton fibers, 60 parts of nanofibers, 20 parts ...
Embodiment 3
[0044] S1, the preparation of outer layer fabric: first select 10 parts of polyester fibers, 15 parts of spandex fibers and 15 parts of acrylic fibers respectively, then carry out scouring, bleaching and mercerizing pre-treatment in sequence with the selected polyester fibers, spandex fibers and acrylic fibers, Then dye the polyester fibers, spandex fibers and acrylic fibers after the pretreatment, then clean the dyed fibers, and then place them in a dryer for drying. The drying temperature is 85°C, and the drying time is set to 2 hours, make the moisture content in the fiber be less than 5%, then the fiber after drying is carried out spinning processing by spinning machine, can obtain the polyester fiber of required color, spandex fiber and acrylic fiber, afterwards polyester fiber, Spandex fiber and acrylic fiber are spun through a blending machine to obtain the outer fabric;
[0045] S2. Preparation of the inner layer fabric: first select 50 parts of cotton fibers, 80 parts...