Embodiment 1
[0012] An environmentally friendly paint, comprising the following components by mass percentage: 3% lemon oil, 2% orange oil, 3% titanium dioxide,
[0013] 1% carbon black, 3% gum modified alkyd resin, 70% Portland cement, 3% water reducer, 2% fly ash, 8% diatomaceous earth, and the rest is solvent.
[0014] The preparation method of the environment-friendly coating comprises the following steps: 1. mixing and stirring lemon oil, orange oil and titanium dioxide at normal temperature;
[0015] 2. Mix the grease modified alkyd resin, portland cement, water reducer, fly ash and diatomaceous earth at room temperature and stir evenly;
[0016] 3. Pour the products obtained in step 1 and step 2 into the mixing tank in proportion, add the solvent, stir slowly, and gradually raise the temperature from 0°C to 20°C to prepare the environmental protection coating