Scheelite flotation collecting agent
A collector and scheelite technology, applied in the field of mineral flotation collectors and flotation collectors, can solve problems such as complex process conditions, and achieve the effects of convenient use, good water solubility, and simple preparation methods
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The scheelite flotation collector of this embodiment is prepared from the following raw materials by weight percentage: 28% of benzohydroxamic acid, 71% of modified fatty acid, and 1% of water glass, which are weighed according to the above weight percentages The raw material is to heat the modified fatty acid to 60°C-70°C, add benzhydroxamic acid and stir, then add water glass and stir for 1 hour, and stir evenly to prepare scheelite flotation collector.
[0024] Using the prepared scheelite flotation collector, the flotation grade of the raw ore is 0.39%, and the obtained titanium concentrate grade reaches 1.28%, and the recovery rate is a good indicator of 88.51%.
Embodiment 2
[0026] The scheelite flotation collector of this embodiment is prepared from the following raw materials by weight percentage: 30% of benzohydroxamic acid, 69% of modified fatty acid, and 1% of water glass, which are weighed according to the above weight percentages The raw material is to heat the modified fatty acid to 60°C-70°C, add benzhydroxamic acid and stir, then add water glass and stir for 1 hour, and stir evenly to prepare scheelite flotation collector.
[0027] Using the prepared scheelite flotation collector, the flotation grade of the raw ore is 0.39%, and the obtained titanium concentrate grade reaches 1.29%, and the recovery rate is a good indicator of 88.38%.
Embodiment 3
[0029] The scheelite flotation collector of this embodiment is prepared from the following raw materials by weight percentage: 32% of benzohydroxamic acid, 67% of modified fatty acid, and 1% of water glass, which are weighed according to the above weight percentages The raw material is to heat the modified fatty acid to 60°C-70°C, add benzhydroxamic acid and stir, then add water glass and stir for 1 hour, and stir evenly to prepare scheelite flotation collector.
[0030] Using the prepared scheelite flotation collector, the flotation grade of the raw ore is 0.39%, and the obtained titanium concentrate grade reaches 1.32%, and the recovery rate is a good indicator of 88.89%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com