An intelligent building and sensor technology, applied in buildings, application of piezoresistive materials, property force measurement, building components, etc., can solve the problems of lack of data detection and analysis, destructive drilling core sampling, bulky testing instruments, etc., to achieve excellent Pressure sensitive performance, excellent electrical conductivity, long service life effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0022] Specific implementation mode 1: This implementation mode is a preparation method of an intelligent building sensor with pressure-sensitive performance, which is specifically carried out according to the following steps:
[0023] 1. Weigh raw materials: Weigh 0.5 to 1 part of graphene oxide, 100 to 110 parts of clay and 30 to 180 parts of deionized water in parts by mass;
[0024] 2. 0.5-1 part of graphene oxide weighed in step 1 is configured into a graphene oxide aqueous solution, and the concentration of the graphene oxide aqueous solution is 20mg / g-30mg / g;
[0025] Then add 30 to 180 parts of deionized water weighed in step 1 to the graphene oxide aqueous solution for dilution, and stir for 10 to 15 minutes to obtain a graphene oxide dilution;
[0026] Add 100 to 110 parts of clay weighed in step 1 to the graphene oxide dilution, stir while adding, and continue stirring for 30 to 40 minutes after the addition to obtain a mixture of graphene oxide and clay;
[0027] ...
specific Embodiment approach 2
[0030] Embodiment 2: This embodiment differs from Embodiment 1 in that: in step 1, 0.7 parts of graphene oxide, 100 parts of clay and 150 parts of deionized water are weighed in parts by mass. Others are the same as the first embodiment.
specific Embodiment approach 3
[0031] Specific embodiment three: the difference between this embodiment and specific embodiment one or two is that in step two, 0.7 parts of graphene oxide weighed in step one is configured into a graphene oxide aqueous solution, and the graphene oxide aqueous solution is The concentration is 25mg / g. Others are the same as those in Embodiment 1 or 2.