[0061] This embodiment includes the following steps:
[0062] 1) Warping: the cotton yarn and the flat yarn are warped separately; the flat yarn is warped as the lower weaving shaft, and the cotton yarn is warped for standby; the cotton yarn warping speed is 200m / min, and the warping tension is 13g; the flat yarn warping speed is 10m / min, warping tension 35g;
[0063] 2) Cotton yarn sizing: the cotton yarn is sizing, sizing, sizing, and then winded into the upper woven shaft after entering the dry splitting area; the viscosity of the cotton fiber sizing tank is 8%, and the sizing rate is 9%; the size is polyvinyl alcohol 3g / L, starch 2.5g / L, acrylic acid 1g / L and water as solvent;
[0064] 3) Weaving: Weaving by air-jet upper and lower shaft looms, the upper and lower weaving shafts are mounted on the loom for heddle and weaving; Alternately pass through the split rods up and down; 3 split rods are arranged in parallel; the cross section of the split rods is elliptical;
...
Embodiment 2
[0068] This embodiment includes the following steps:
[0069] 1) Warping: the cotton yarn and the flat yarn are warped separately; the flat yarn is warped as the lower weaving shaft, and the cotton yarn is warped for standby; the cotton yarn warping speed is 205m / min, and the warping tension is 12g; the flat yarn warping speed is 5 m / min, warping tension 34g;
[0070] 2) Cotton yarn sizing: the cotton yarn is sizing, sizing, sizing, and then winded into the upper woven shaft after entering the dry splitting area; the viscosity of the cotton fiber sizing tank is 6%, and the sizing rate is 8%; the size is polyvinyl alcohol 3g / L, starch 2.5g / L, acrylic acid 1g / L and water as solvent;
[0071] 3) Weaving: Weaving by air-jet upper and lower shaft looms, the upper and lower weaving shafts are mounted on the loom for heddle and weaving; Alternately pass through the split rods up and down; 4 split rods are arranged in parallel; the cross section of the split rods is circular;
[...
Embodiment 3
[0075] This embodiment includes the following steps:
[0076] 1) Warping: The cotton yarn and the flat yarn are warped separately; the flat yarn is warped as the lower weaving shaft, and the cotton yarn is warped for standby; the cotton yarn warping speed is 190m / min, and the warping tension is 14g; the flat yarn warping speed is 10m / min, warping tension 32g;
[0077] 2) Cotton yarn sizing: the cotton yarn is sizing, sizing, sizing, and then winded into the upper woven shaft after entering the dry splitting area; the viscosity of the cotton fiber sizing tank is 7%, and the sizing rate is 8.6%; the size is 3g of polyvinyl alcohol / L, starch 2.5g / L, acrylic acid 1g / L and water as solvent;
[0078] 3) Weaving: Weaving by air-jet upper and lower shaft looms, the upper and lower weaving shafts are mounted on the loom for heddle and weaving; Alternately pass through the split rods up and down; 3 split rods are arranged in parallel; the cross section of the split rods is circular;...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com