Manufacturing method of light and thin alloy vibrating diaphragm
A manufacturing method and alloy technology, which is applied in the field of diaphragm manufacturing, can solve the problems of poor bonding force, weak corrosion resistance, and high defect rate of PeeK, and achieve the effects of high bonding stability, convenient operation, and high yield rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Method for manufacturing a lightweight alloy diaphragm, which includes the following steps:
[0028] (a) Alloy material is prepared, and the pollutant on the workpiece is softened, separated, and dissolved by using an organic solvent coating.
[0029] (b) Use the improving product band required to be improving;
[0030] (c) Organic solvent removal oxidation layer;
[0031] (d) Cleaning to peel off the surface of the surface of the workpiece;
[0032] (g) A single piece from the product with the secondary processing of the product.
[0033] The light-thin alloy diaphragm manufacturing method also includes step (e): a low pressure hot air drying in a whole direction, wherein step (e) is before (g) and after step (d).
[0034] The light-thin alloy diaphragm manufacturing method also includes step (f): electrophoresis of the product, wherein step (f) is before (G) and is behind step (e).
[0035] The method of manufacturing the lightweight alloy diaphragm also includes step (h)...
Embodiment 2
[0037] Such as figure 1 As shown, a method of manufacturing a lightweight alloy diaphragm comprising the steps of:
[0038] (a) Alloy material is prepared, and the pollutant on the workpiece is softened, separated, and dissolved, dissolved, and dissolved to form a metal belt 11 using an organic solvent coating method.
[0039] (b) Forming a metal strip 11 using a flush molded mold 11 to form a product belt 12, a product belt comprises a tape 121, a material tape hole 122, and a product 123;
[0040] (c) Organic solvent removes the oxide layer of the product strap 12;
[0041] (d) Cleaning the soil peeling of the surface of the product strip 12 surface;
[0042] (e) The low-voltage hot air drying product belt 12 is performed in a full range from top to bottom.
[0043] (f) Take the product 12 electrophoresis;
[0044] (g) Make the product secondary processing from the product with a single piece product 123.
[0045] The light-thin alloy diaphragm manufacturing method also includes...