Bubble mixed light clay and method for preparing the same
A production method and light soil technology, which is applied in the field of air bubble mixed light soil, can solve the problems of increased construction cost, large volume of fly ash soil, high cost, etc., and achieve the effects of uniform filling, easy construction of filling soil, and high fluidity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] 1. Take 400Kg of sandy soil from which debris such as large stones and bricks have been removed;
[0033] 2. Take 300Kg of pozzolan cement and 270Kg of mixed water, pour the three components into the mixer and mix them evenly; the pozzolan cement mainly plays the role of consolidation and strengthening the skeleton of the soil, and the same amount of ordinary silicate can also be used for pozzolan cement Cement or blast furnace Portland cement, etc., after these materials are added to the soil, water will react with water to produce Ca(OH) 2 Product, Ca(OH) 2 Ion exchange with clay particles to form a solidified product, to achieve the role of strengthening the skeleton of the soil. In addition, a curing auxiliary agent for the purpose of catalysis and early setting is added to the above cement. The curing auxiliary agent is fly ash, gypsum powder or silicon powder, etc. The purpose of adding these materials is also to reduce the amount of cement. Add 50Kg of fly ash ...
Embodiment 2
[0036] Directly take 550Kg of ordinary Portland cement and 400Kg of mixed water and pour them into the blender to stir and mix evenly; add 50Kg of air bubbles to the mixture and let the air bubbles evenly distribute in the mixture by stirring to obtain air bubbles that can be used for pouring immediately Mix in light soil. In a dry state, the pore volume formed by air bubbles in the light soil mixed with air bubbles in this embodiment accounts for about 65% of the total volume.
Embodiment 3
[0038] Take 660Kg of sandy soil, 120Kg of blast furnace Portland cement, and 210Kg of mixed water, pour the three components into the mixer and mix them evenly; then add 10Kg of air bubbles to the mixture and let the air bubbles evenly distribute in the mixture by stirring In the process, air-mixed light soil that can be used for pouring immediately is obtained. In a dry state, the volume of pores formed by air bubbles in the light soil mixed with air bubbles in this embodiment accounts for about 40% of the total volume.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com