Method for manufacturing wool top, Qinglun and Jinlun interweaving wool
A manufacturing method and technology for tops, applied in textiles, papermaking, yarn, etc., can solve the problems of unsuitable wearing of chemical fibers, easy generation of static electricity, high manufacturing cost, etc., and achieve the effect of safe and healthy wearing, no toxic side effects, and low manufacturing cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] 20% wool top, 20% acrylic, and 60% nylon are mixed and processed, firstly needled (head needle, two needles, three needles, four needles), then needled on a roving frame, and then wetted at a constant temperature. Wet time: 24 hours, the temperature is controlled at 24°C, and then spun on the spinning frame to meet the setting standard, the standard is 7.6-56 counts, and the above-mentioned spun yarn that meets the setting standard is stored at a constant temperature, and the storage temperature is controlled at 23°C-24°C , the time is 11 hours, and then the stored spun yarn is dropped into the single cylinder for two strands and twisting, and then the wool joint car is combined and twisted for three strands, and the yarn is shaken, dyed, and finally formed into a ball. This product is .
Embodiment 2
[0014] Take 50% of wool, 30% of nylon and 20% of acrylic and process it through mixing. Firstly, go through needle combing (head needle, two needles, three needles, four needles), and then go through needle combing on the roving frame, and then apply humidity at constant temperature, and then give moisture at constant temperature. Wet time: 25 hours, the temperature is controlled at 24°C, and then spun on the spinning frame until it meets the setting standard, the standard is 7.6-56 counts, and the above-mentioned spun yarn that meets the setting standard is stored at a constant temperature, and the storage temperature is controlled at 23°C. The time is 13 hours, and then the stored spun yarn is dropped into a single cylinder for two strands and twisting, and three yarns are combined and twisted on the pile yarn joint car, shaken, dyed, and finally balled into this product.
Embodiment 3
[0016] 30% of wool, 40% of acrylic and 30% of nylon are mixed. And adopt embodiment 1, 2 manufacturing process processing method, the constant temperature humidity supply time is 24.5 hours, the temperature is 24.5 ℃, the constant temperature storage time is 12 hours, the temperature is 24.5 ℃, the velvet made also meets the above-mentioned standard.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com