Embodiment 1
[0019] Weigh 85.66 grams of PY138, 0.82 grams of PG7, 10.56 grams of PY153, 39.33 grams of PW6, and 1000 grams of CSC-C base material. Mix the above raw materials, and then apply the mixed composition evenly and evenly on the coated paper under the environmental conditions of relative humidity of 50%±5% and room temperature of 23±2°C. The wet film thickness of the coating is 250 μm, and then placed in a precision oven at 50±2°C for 3 to 4 hours to constant weight, taken out, cooled to room temperature, and obtained a physical color block.
Embodiment 2
[0020] Example 2: Weigh 84.66 grams of PY138, 0.80 grams of PG7, 11 grams of PY153, 39 grams of PW6, and 1000 grams of CSC-C base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0021] Example 3: Weigh 86.66 grams of PY138, 0.82 grams of PG7, 10.57 grams of PY153, 39.33 grams of PW6, and 1005 grams of CSC-C base material. Manufacturing process is with embodiment 1.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| minimum film forming temperature | aaaaa | aaaaa |
| glass transition temperature | aaaaa | aaaaa |