High ornamental environment-friendly type integral seamless grinding stone terrace and manufacturing technique thereof
A manufacturing process and decorative technology, which is applied in the field of highly decorative and environmentally friendly integral seamless terrazzo flooring and its manufacturing process, can solve the problem of not meeting the requirements of decoration, lack of appreciation value and aesthetic effect, and inability to design Art pattern floor and other problems, to achieve the effect of rich and changeable pattern color and shape, wear resistance and service life, and good adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Embodiment 1: A highly decorative and environmentally friendly integral seamless terrazzo floor and its manufacturing process are realized according to the following steps: use a grinder to polish and vacuum the floor, and use epoxy resin grouting for consolidation after the loose structure is consolidated. Solvent epoxy varnish primer, the amount of primer is 0.2kg / m 2;After the primer is cured, use solvent-free epoxy mortar paint to scrape the sand again. The mortar paint contains 35% of 20-40 mesh coarse sand and 15% of 60-80 mesh fine sand; after the first mortar paint is cured After 6 hours, scrape and coat the mortar paint for the second time. The second mortar paint material contains 35% of 60-80 mesh quartz sand and 15% of 150-200 mesh quartz powder; after the second mortar layer is cured for 8 hours According to the design pattern, the metal mold is bonded to the mortar layer with epoxy glue, and the paving machine is poured into the mold to spread the solvent-...
Embodiment 2
[0020] Example 2: A highly decorative and environmentally friendly integral seamless terrazzo floor and its manufacturing process are realized according to the following steps: use a grinder to polish and vacuum the floor, and use epoxy resin grouting for consolidation after the loose structure is water-based Epoxy varnish primer, the amount of primer is 0.15kg / m 2 ; After the primer is cured, scrape the sand once with water-based epoxy mortar paint, which contains 35% of 60-80 mesh quartz sand and 15% of 150-200 mesh quartz powder; wait for the mortar layer to cure for 8 hours Finally, the metal mold is bonded to the mortar layer with epoxy glue according to the design pattern, and the solvent-free epoxy grindstone floor slurry is poured into the mold with a paver. The composition is: liquid epoxy resin 28% , 2% epoxy reactive diluent, 15% supporting solvent-free amine curing agent, 2% green toner, 53% crushed colored stones. Use a walk-behind trowel to mechanically vibrate ...
Embodiment 3
[0021] Example 3: A highly decorative and environmentally friendly integral seamless terrazzo floor and its manufacturing process are realized according to the following steps: use a grinder to grind and vacuum the floor, and use epoxy resin grouting for consolidation after the loose structure is water-based Epoxy varnish primer, the amount of primer is 0.15kg / m 2 After the primer is cured, use solvent-free epoxy mortar paint to scrape sand again. The mortar paint contains 40% of 60-80 mesh quartz sand and 20% of 150-200 mesh quartz powder; wait for the mortar layer to cure for 8 hours Finally, according to the design pattern, the plastic mold is glued to the mortar layer with super glue, and the paver is used to pour and spread the solvent-free epoxy grindstone floor slurry into the mold. The composition is: 16% liquid epoxy resin, 2% epoxy reactive diluent, 9% supporting solvent-free amine curing agent, 2% pink powder, 71% grinding stone aggregates such as broken shells, gla...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com