[0012] Example 1
[0013] First pour 30% water into the dispersing kettle, keep the dispersing speed 500-700 rpm, then add 3% extracts of aloe vera, Tian Qi, and peppermint to the dispersing kettle, disperse for 3-5 minutes, and then add 10% sequentially Titanium dioxide, 30% powder filler, dispersed for 10-15 minutes at a speed of 1500-2000 rpm, then injected into the grinder for grinding, then added 27% emulsion, dispersed for 5-10 minutes, and finally carried out viscosity and contrast ratio , Inspection of regular indicators of fineness and constructability, and packaging and storage after qualified.
Example Embodiment
[0014] Example 2
[0015] First inject 30% water into the dispersing kettle, maintain the dispersing speed at 500-700 rpm, then add 5% of the extracts of aloe vera, Tianqi and peppermint to the dispersing kettle, disperse for 3-5 minutes, and then add 12% in turn Titanium dioxide, 28% powder filler, dispersed for 10-15 minutes at a speed of 1500-2000 rpm, then injected into the grinder for grinding, then added 25% emulsion, dispersed for 5-10 minutes, and finally carried out viscosity and contrast ratio , Inspection of regular indicators of fineness and constructability, and packaging and storage after qualified.
Example Embodiment
[0016] Example 3
[0017] First inject 30% water into the dispersing kettle, keep the dispersing speed 500-700 rpm, then add 8% aloe vera, Tianqi, and peppermint extracts into the dispersing kettle, disperse for 3-5 minutes, and then add 15% sequentially Titanium dioxide, 22% powder filler, dispersed for 10-15 minutes at a speed of 1500-2000 rpm, then injected into the grinder for grinding, then added 25% emulsion, dispersed for 5-10 minutes, and finally carried out viscosity and contrast ratio , Inspection of regular indicators of fineness and constructability, and packaging and storage after qualified.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap