Non-nicotine like-tobacco product and preparation method thereof
A nicotine-free and tobacco-free technology, which is applied in the fields of tobacco, tobacco processing, and cigar manufacturing, can solve problems such as harm to the human body and high nicotine toxicity, and achieve the effect of eliminating harm, avoiding harm to human health and low cost.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0016] The preparation method of the nicotine-free tobacco product of the present invention is as follows: first drying the plant fiber, processing it into shreds, then shredding the tea leaves, mixing them evenly with taste seasonings and glycerin, and then rolling the finished product by using cigarette equipment.
[0017] Taste seasoning can be sweetener or essence or spices etc., can add according to actual needs.
[0018] The specific technological process of the above-mentioned nicotine-free e.g. tobacco product preparation method can be carried out as follows:
[0019] a. Dry the plant fiber, and then process it into silk: the silk strips with a width of 0.8-1.0mm and a length of 3-10mm are used for later use.
[0020] b. Adopt qualified tea leaves (such as oolong tea), cut them into strips with a width of 0.8-1.0mm and a length of 3-10mm with shredding equipment for later use.
[0021] c. Mix the processed plant fiber, tea shreds, taste seasoning, and glycerin evenly,...
Embodiment 1
[0023] In the nicotine-free tobacco product of the present invention, each component is mixed with the following percentages by weight: 60% plant fiber, 10% tea, 29% mouthfeel seasoning, and 1% glycerin. Rolled cost products.
Embodiment 2
[0025] The specific process of the preparation method of the nicotine-free tobacco product of the present invention can be carried out as follows:
[0026] a. Dry the plant fiber, and then process it into silk: the width of the thread is 0.8-1.0mm, the length of the thread is 3-10mm, and it is used for later use.
[0027] b. Adopt qualified tea leaves (such as oolong tea), cut into strips with shredding equipment: strip width 0.8-1.0mm, strip length 3-10mm, set aside.
[0028] c. Mix the processed plant fiber, tea shreds, taste seasoning, and glycerin evenly, and roll the product with cigarette equipment.
PUM
Property | Measurement | Unit |
---|---|---|
Width | aaaaa | aaaaa |
Length | aaaaa | aaaaa |
Width | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com