Aqueous compound anti-counterfeit paint for paper as well as preparation method and application thereof
A water-based and coating technology, applied in papermaking, pigmented coatings, textiles and papermaking, etc., can solve problems such as difficult to apply, non-high-tech anti-counterfeiting coatings, and easy exposure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A water-based composite anti-counterfeiting coating for paper, its preparation raw materials include the following mass ratio components, 20 parts of capsule-type reversible temperature-changing color powder (NCC, red, color-changing temperature 40°C); capsule-type sunlight reversible color powder (NCC, green) 20 parts; liquid ultraviolet fluorescent agent (APC, blue fluorescent) 1 part; infrared fluorescent powder (RL-801, yellow fluorescent) 10 parts; metal inorganic salt (potassium sulfate) 2 parts; PD starch glue 5 parts ; 42 parts of water.
[0013] Preparation of composite water-based paint: 1. Add 42 parts of water into a container with adjustable frequency conversion stirring, start stirring, stirring speed 300~500rpm / min, add 5 parts of PD starch glue, heat up to 90~95℃, keep warm 20~30min, then cool down to 50~55°C; 2. Adjust the stirring speed to 1000~1200 rpm / min, add 20 parts of thermochromic powder, 20 parts of photochromic powder, 10 parts of infrared flu...
Embodiment 2
[0023] A water-based composite anti-counterfeiting coating for paper, its preparation raw materials include the following mass ratio components, 18 parts of capsule-type reversible temperature-changing color powder (NCC, green, color-changing temperature 50°C); capsule-type sunlight reversible color powder (NCC, blue) 16 parts; liquid ultraviolet fluorescent agent (APC, blue fluorescent) 2 parts; infrared fluorescent powder (RL-801, red fluorescent) 12 parts; metal inorganic salt (barium chloride) 3 parts; PD starch glue 6 parts; 45 parts of water.
[0024] Prepare composite water-based paint according to the above composition: 1. Add 45 parts of water into a container with adjustable frequency conversion stirring, start stirring, and stir at a speed of 300~500rpm / min, add 6 parts of PD starch glue, and heat up to 90~95 ℃, keep warm for 20~30min, then cool down to 50~55℃; 2. Adjust the stirring speed to 1000~1200 rpm / min, add 18 parts of thermochromic powder, 16 parts of optic...
PUM
| Property | Measurement | Unit |
|---|---|---|
| solid content | aaaaa | aaaaa |
| solid content | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com