Laminate flooring colorized solid sealing wax and preparation method thereof

A kind of laminate flooring and color technology, which is applied in the direction of chemical instruments and methods, and other chemical processes, can solve the problems of uneven surface color, black base material at the floor splicing, and affect the overall appearance of the floor, so as to improve the overall appearance , the effect of uniform color

Inactive Publication Date: 2012-08-08
JIAXING UNIV +1
View PDF2 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, for the laminate flooring treated with wax seal, the wax seal cannot effectively cover the base material at the floor lock due to the transparency of the wax; moreover, due to the high permeability of paraffin wax, the color of the seam and the floor surface are not uniform , and make the base material of the floor splicing black, affecting the overall appearance of the floor

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

preparation example Construction

[0024] The preparation method of the colored solid sealing wax for laminate flooring is as follows: Weigh the required raw materials in proportion, melt and mix the raw materials, and then cool. The steps of melting and mixing are as follows:

[0025] (A) dissolving the surface modifier in 5-20 times the weight of ethanol, then spraying it on the surface of the powdery polymer material, stirring evenly; then drying it in a vacuum oven at 50°C for 3-5 hours;

[0026] (B) heating and melting the polymer material obtained in step A, and mixing it with the organic pigment;

[0027] (C) heating, melting and mixing the material obtained in step B with paraffin.

Embodiment 1

[0029] The components used in this embodiment are as follows:

[0030] Microcrystalline Wax 70%, Polyethylene Wax 22%,

[0031] Toluidine Red 4%, Span-60 4%.

[0032] making process:

[0033] (A) Dissolve Span-60 in 10 times the weight of ethanol, then spray on the surface of the powdery polyethylene wax, and stir while dispersing; then place the polyethylene wax after the surfactant treatment at 50°C Dry in a vacuum oven for 4 hours;

[0034] (B) Melt the dried polyethylene wax at 120°C, add toluidine red in the molten state, stir and mix evenly;

[0035] (C) In molten state, add paraffin and stir well.

[0036] (D) After cooling, the colored solid sealing wax for laminate flooring is obtained.

Embodiment 2

[0038] The components used in this embodiment are as follows:

[0039] Microcrystalline Wax 85%, Polyethylene Wax 10%,

[0040] Phthalo Blue 2%, Span-60 3%.

[0041] In the preparation process (A), dry in a vacuum oven for 5 hours, and the rest are the same as in Example 1.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

A laminate flooring colorized solid sealing wax comprises, by weight, 50-85% of paraffin, 10-45% of a polymer material, 1-8% of an organic pigment, and 1-8% of a surface modifier. A preparation method of the laminate flooring colorized solid sealing wax comprises the following steps: weighing required raw materials according to above proportions, fuse-mixing the raw materials, and cooling. Lock catches of wood floors processed with the laminate flooring colorized solid sealing wax have moisture-proof lubrication effects of the lock catches of the floors processed with traditional paraffin, and the colorized solid sealing wax is configured according to the color of the floor surface to unify the floor in color to effectively cover base materials at the lock catches of the floors, so a uniform color effect is obtained, and the overall aesthetic degree of the floor is greatly improved.

Description

technical field [0001] The invention relates to a technique for strengthening solid sealing wax used for locks of wooden floors, a colored solid sealing wax for strengthening wooden floors and a preparation method thereof. Background technique [0002] In recent years, with the continuous development of the timber market and the improvement of people's living standards, wooden flooring has gradually entered thousands of households. In order to obtain a bright, moisture-proof, and uniformly colored floor surface, paint treatment is generally performed on the floor surface. However, only the surface paint treatment of laminate flooring is not enough. The humid environment will cause deformation and expansion of the floor after splicing. Therefore, sealing wax is generally used at the floor lock to achieve moisture-proof and lubricating effects. However, for the laminate flooring treated with wax seal, the wax seal cannot effectively cover the base material at the floor lock d...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C08L91/06C08L23/06C08L77/00C08L27/18C08L23/12C08J3/20C09K3/10
Inventor 屠晓华吴建一倪庆一缪程平沈静飞陈利
Owner JIAXING UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products