Problems solved by technology
Method used
Examples
Embodiment 1
[0052] Example 1 Production of 80㎝×80㎝ oil paintings with 3㎜ embossed relief
[0053] A method for large-scale production of embossed decorative paintings, mainly comprising the following steps:
[0054] (1) Material selection, select PMMA material, the material thickness is 1.8mm, the shrinkage rate is <1%, and the material thickness tolerance is <6%.
[0055] (2) To make a mold, the size of the mold is 80㎝-1.8㎜×2 in length, 80㎝-1.8㎜×2 in width, and the unevenness of the mold relief is 3㎜.
[0056] (3) For forming, first heat the selected PMMA material to 90°C, then cover the heated material on the mold, start the blister machine, form, and demould when the temperature drops to 50°C.
[0057] (4) Surface treatment, put the formed product on the spray table of the UV inkjet printer, align the position, start the machine, and the inkjet printing is completed.
[0058] (5) Adhesive bottom plate mounting, put the painted product into the selected oil painting frame, cover the...
Embodiment 2
[0059] Example 2 Production of 80cm×200cm imitation precious metal calligraphy and painting
[0060] A method for large-scale production of embossed decorative paintings, mainly comprising the following steps:
[0061] (1) Material selection, choose PVC material, the material thickness is 2.5mm, the shrinkage rate is <0.7%, and the material thickness tolerance is <4%.
[0062] (2) To make a mould, the size of the mold does not need to be scaled. The male mold is first made, and then the female mold is made. The male mold is placed in the female mold with a gap of 2.5 mm. The clamping mold is fixed in a good position in the extrusion machine.
[0063] (3) Forming, heat the selected PVC material to 80°C and place it on the top of the female mold, start the machine, let the male mold press down, and remove the male mold when the temperature drops to 45°C.
[0064] (4) Surface treatment: wash and dry the surface of the formed product, and use vacuum plating technology to carry ...
Embodiment 3
[0066] Example 3 Produce 100cm×240cm imitation woodcarving products with a relief unevenness of 5cm
[0067] A method for large-scale production of embossed decorative paintings, mainly comprising the following steps:
[0068] (1) Material selection, choose ABS material, the material thickness is 3 mm, the shrinkage rate is <0.7%, and the material thickness tolerance is <4%.
[0069] (2) To make a mould, the size of the mold does not need to be scaled. The male mold is made first, and then the female mold is made. The male mold is placed in the female mold, and there is a gap of 3mm. The clamping mold is fixed in a good position in the extrusion machine.
[0070] (3) For molding, heat the selected ABS material to 105°C and place it on the top of the female mold, start the machine, let the male mold press down, and remove the male mold when the temperature drops to 45°C.
[0071] (4) Surface treatment, lay the formed product flat, cover it with the selected wood grain PVC fi...
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com