Paraffin sizing agent and preparation method thereof
A sizing agent and paraffin technology, applied in the direction of adding water repellents, etc., can solve the problems of low sizing degree of paraffin sizing agent and low paper surface strength, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A preparation method of a paraffin wax sizing agent, the preparation method comprising the following steps: (1) take 15 kg of paraffin wax, 7 kg of methyl glucose dioleate, and 5 kg of diethylene glycol monolaurate, and heat the paraffin wax , methyl glucose dioleate, and diethylene glycol monolaurate were stirred and dissolved; (2) Take 3kg of sodium alginate, 4kg of oxidized starch, and 134kg of deionized water, and mix sodium alginate with oxidized Stir and dissolve the starch with deionized water; (3) Mix the mixture in step (1) and step (2), then add polyvinyl alcohol to 3kg, and stir evenly; (4) After stirring evenly, use a shearing machine to cut Cutting treatment, the shearing speed is 4500rpm, and the shearing time is 15min. The solid content of the prepared paraffin wax sizing agent was 19.2wt%.
Embodiment 2
[0014] A kind of preparation method of paraffin wax sizing agent, preparation method comprises the following steps: (1) take paraffin wax as 17kg, methyl glucose dioleate as 4kg, diethylene glycol monolaurate as 6kg, paraffin wax after heating , methyl glucose dioleate, and diethylene glycol monolaurate were stirred and dissolved; (2) Take 3kg of sodium alginate, 5kg of oxidized starch, and 130kg of deionized water, and mix sodium alginate with oxidized Stir and dissolve the starch with deionized water; (3) Mix the mixture in step (1) and step (2), then add polyvinyl alcohol to 4kg, and stir evenly; (4) After stirring evenly, use a shearing machine to cut Cutting treatment, the shearing speed is 4500rpm, and the shearing time is 25min. The solid content of the prepared paraffin wax sizing agent was 22.1wt%.
Embodiment 3
[0016] A preparation method of a paraffin wax sizing agent, the preparation method comprising the following steps: (1) take 18 kg of paraffin wax, 5 kg of methyl glucose dioleate, and 5 kg of diethylene glycol monolaurate, heat the paraffin wax , methyl glucose dioleate, and diethylene glycol monolaurate were stirred and dissolved; (2) Take 4kg of sodium alginate, 5kg of oxidized starch, and 132kg of deionized water, and mix sodium alginate with oxidized Stir and dissolve the starch with deionized water; (3) Mix the mixture in step (1) and step (2), then add polyvinyl alcohol to 2kg, and stir evenly; (4) After stirring evenly, use a shearing machine to cut Cutting treatment, the shearing speed is 4500rpm, and the shearing time is 20min. The solid content of the prepared paraffin wax sizing agent was 20.5wt%.
[0017] Get the paraffin wax sizing agent of embodiment 1, embodiment 2, embodiment 3 and dilute to 12wt% with water, get common white cardboard and immerse in the paraf...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com