A treatment method and technology of poplar bark, applied in wood treatment, pretreatment equipment, wood treatment details, etc., can solve the problems of bark deformation and cracking, affecting the value of bark painting, etc., to improve quality, make coloring and painting easy, and paint stable effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] A processing method for poplar bark used for bark painting, using the following steps:
[0012] Mix and stir 3.2 parts of polyethylene glycol and 20 parts of water to dissolve them, then add 9 parts of glycerin to the mixed solution to mix evenly, add 2.8 parts of paraffin oil, 9 parts of ethanol, 2.5 parts of sodium benzenesulfonate, six Stir 2 parts of sodium metaphosphate to make it fully mixed, then add 7.2 parts of potassium nitrate to mix and dissolve to obtain a treatment solution;
[0013] Peel off the whole piece of fresh poplar bark, use 2.5% by weight baking soda solution to wash off the mucus on the poplar bark surface, then rinse it with clean water, air-dry the moisture on the poplar bark surface, and then use the above steps to remove the poplar bark The obtained treatment solution is soaked at 28-35°C for 1-3 days, the number of soaking days is determined by the size and thickness of the poplar bark, taken out, rinsed with clean water, air-dried and then...
Embodiment 2
[0015] The treatment solution is formulated by weight from the following raw materials: 2.4 parts of sodium benzenesulfonate, 7.8 parts of glycerin, 6.2 parts of potassium nitrate, 2.8 parts of polyethylene glycol, 2.5 parts of paraffin oil, 2 parts of sodium hexametaphosphate, water 20 parts, 9 parts of ethanol.
Embodiment 3
[0017] The treatment solution is prepared by weight from the following raw materials: 2.4 parts of sodium benzenesulfonate, 8.6 parts of glycerin, 6 parts of potassium nitrate, 3 parts of polyethylene glycol, 2.7 parts of paraffin oil, 2 parts of sodium hexametaphosphate, water 20 parts, 9 parts of ethanol.