A kind of water-based floor paint and preparation method thereof
A floor paint, water-based technology, applied in coatings, cellulose coatings, polyester coatings, etc., can solve the problems of difficult production process, high TDI toxicity, high production cost, achieve good environmental performance, protect health, flow high level effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Preparation of component A: Add 587 kg of curing agent into the stirring container, add 10 kg of wetting agent, 6 kg of defoamer, and 7 kg of dispersant in sequence under low-speed stirring (400rmp), and stir for 10 minutes, then add while stirring 160kg of titanium dioxide, high-speed dispersion (1000rmp) for 30 minutes to make a dispersion slurry, after the fineness is qualified, change to medium-speed stirring (600rpm), add 150kg of deionized water, 6kg of defoamer, 6kg of thickener, 8kg of leveling Agent and 60kg color paste, after stirring for 15 minutes, pass the test, filter and pack, it is component A. Mix component A and component B in a ratio of 1:2.5 to get water-based floor paint.
Embodiment 2
[0030] Preparation of component A: Add 634 kg of curing agent into the stirring container, add 10 kg of wetting agent, 6 kg of defoamer, and 10 kg of dispersant in sequence under low-speed stirring (400rmp), and stir for 10 minutes, then add while stirring 180kg of titanium dioxide, high-speed dispersion (1000rmp) for 30 minutes to make a dispersion slurry, after the fineness is qualified, change to medium-speed stirring (600rpm), add 100kg of deionized water, 6kg of defoamer, 6kg of thickener, 8kg of leveling Agent and 40kg color paste, after stirring for 15 minutes, pass the test and then filter and package, which is component A. Mix component A and component B in a ratio of 1:2.7 to get water-based floor paint.
Embodiment 3
[0032] Preparation of component A: Add 685 kg of curing agent into the stirring container, add 10 kg of wetting agent, 6 kg of defoamer, and 10 kg of dispersant in sequence under low-speed stirring (400rmp), and stir for 10 minutes, then add while stirring 124kg of titanium dioxide, high-speed dispersion (1000rmp) for 30 minutes to make a dispersion slurry, after the fineness is qualified, change to medium-speed stirring (600rpm), add 80kg of deionized water, 6kg of defoamer, 3kg of thickener, 6kg of leveling Agent and 70kg color paste, after stirring for 15 minutes, pass the test, filter and pack, it is component A. Mix component A and component B in a ratio of 1:3.0 to get water-based floor paint.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com