A dyeing method, the technology of bubble fleece, which is applied in the direction of dyeing, textiles and papermaking, etc., can solve the problems of low color fastness of dyed fabrics, poor dyeing uniformity, easy to produce colored flowers, etc., and achieve good dyeing uniformity , Excellent color fastness to washing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] The dyeing method of bubble fleece fabric, comprises the steps:
[0040] 1) Add 1 to 2 parts by weight of octadecyldimethylamine, 1.2 parts by weight of sodium sulfate, 2.6 parts by weight of sodium pyrophosphate, 0.5 parts by weight of ammonia water, and 20 parts by weight of vegetable dyes in turn in 100 parts by weight to the dye vat. Ionized water, stir evenly, and heat to 45°C;
[0041] 2) Add 0.8 parts by weight of sodium ethylenediamine tetramethylene phosphonate, 2.1 parts by weight of sodium α-alkenyl sulfonate, 1.1 parts by weight of methallylamine hydrochloride, and 0.4 parts by weight of zinc stearate , continue to stir until fully mixed and heated to 60°C;
[0042] 3) Soak the fabric in the dye vat for 40 minutes;
[0043] 4) drying the soaked fabric at 85°C;
[0044] 5) soak the dried fabric in clean water and rinse for 40 minutes;
[0045] 6) Take out the rinsed fabric and let it dry naturally.
Embodiment 2
[0047] The dyeing method of bubble fleece fabric, comprises the steps:
[0048] 1) Add 1 part by weight of octadecyldimethylamine, 1.2 parts by weight of sodium sulfate, 2.6 parts by weight of sodium pyrophosphate, 0.5 parts by weight of ammonia water, and 20 parts by weight of vegetable dyes into 100 parts by weight of deionized water in turn in the dye vat , stir evenly, and heat to 45°C;
[0049] 2) Add 0.8 parts by weight of sodium ethylenediamine tetramethylene phosphonate, 2.1 parts by weight of sodium α-alkenyl sulfonate, 1.1 parts by weight of methallylamine hydrochloride, and 0.4 parts by weight of zinc stearate , continue to stir until fully mixed and heated to 60°C;
[0050] 3) Soak the fabric in the dye vat for 40 minutes;
[0051] 4) drying the soaked fabric at 85°C;
[0052] 5) soak the dried fabric in clean water and rinse for 40 minutes;
[0053] 6) Take out the rinsed fabric and let it dry naturally.
Embodiment 3
[0055] The dyeing method of bubble fleece fabric, comprises the steps:
[0056] 1) Add 2 parts by weight of octadecyldimethylamine, 1.2 parts by weight of sodium sulfate, 2.6 parts by weight of sodium pyrophosphate, 0.5 parts by weight of ammonia water, and 20 parts by weight of vegetable dyes into 100 parts by weight of deionized water in turn in the dye vat , stir evenly, and heat to 45°C;
[0057] 2) Add 0.8 parts by weight of sodium ethylenediamine tetramethylene phosphonate, 2.1 parts by weight of sodium α-alkenyl sulfonate, 1.1 parts by weight of methallylamine hydrochloride, and 0.4 parts by weight of zinc stearate , continue to stir until fully mixed and heated to 60°C;
[0058] 3) Soak the fabric in the dye vat for 40 minutes;
[0059] 4) drying the soaked fabric at 85°C;
[0060] 5) soak the dried fabric in clean water and rinse for 40 minutes;
[0061] 6) Take out the rinsed fabric and let it dry naturally.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com