An electric water heater and thermal insulation technology, applied in water heaters, fluid heaters, lighting and heating equipment, etc., can solve the problems of reduced thermal insulation performance, little difference in water temperature, poor antibacterial ability, etc. The effect of production efficiency and good closed cell rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Prepare 3 parts by weight of polyether 3050, 10 parts of polyether 4110, 8 parts of polyether 2043, 0.3 part of trifluoropropyl silicone oil, 5 parts of water, 1 part of pozzolan, 3 parts of asbestos wool, 0.1 part of crosslinking agent BDO, 0.3 parts of foaming catalyst and 4 parts of flame retardant magnesium hydroxide. The foaming catalyst uses copper isooctanoate, substituted-4-pyrimidine formate and Dabco TMR-4 with a mass ratio of 1-3; Parts are mixed, then poured into the cavity of the water heater tank for foaming, and the water heater insulation layer used in the present invention can be obtained after curing at high temperature.
Embodiment 2
[0034] Prepare 5 parts of polyether 3050, 15 parts of polyether 4110, 15 parts of polyether 2043, 0.5 parts of trifluoropropyl silicone oil, 8 parts of water, 2 parts of pozzolan, 6 parts of asbestos wool, and 0.2 parts of crosslinking agent EG in parts by weight , 0.5 parts of foaming catalyst and 6 parts of flame retardant magnesium hydroxide. The foaming catalyst uses copper isooctanoate, substituted-4-pyrimidine formate and Dabco TMR-4 with a mass ratio of 3:2:7; 1.5 parts of isocyanate are mixed, then poured into the cavity of the water heater tank for foaming, and after curing at high temperature, the water heater insulation layer used in the present invention is obtained.
Embodiment 3
[0036] Prepare 4 parts of polyether 3050, 13 parts of polyether 4110, 12 parts of polyether 2043, 0.4 part of trifluoropropyl silicone oil, 6 parts of water, 1.5 parts of pozzolan, 5 parts of asbestos wool, 0.15 part of crosslinking agent DEG, 0.4 parts of foaming catalyst and 5 parts of flame retardant magnesium hydroxide. The foaming catalyst uses copper isooctanoate, substituted-4-pyrimidine formate and Dabco TMR-4 with a mass ratio of 2:2:7; the above raw materials are mixed uniformly to form a polyether composition, and then mixed with 1.2 parts of isocyanate are mixed, then poured into the cavity of the water heater tank for foaming, and after curing at high temperature, the water heater insulation layer used in the present invention is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com