Preparation method of triethyl phosphite
A technology of triethyl phosphite and ethanol, applied in the field of preparation of triethyl phosphite, can solve the problems of low yield of triethyl phosphite, unrecoverable, complicated process, etc., and achieves high production efficiency , Easy to recycle, avoid secondary pollution effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A preparation method of triethyl phosphite, its raw materials are as follows by weight: 3 milliliters of ethanol, 1 milliliter of phosphorus trichloride, 3 milliliters of dimethyl aniline, 12 milliliters of petroleum ether.
[0022] Described ethanol is dehydrated alcohol.
[0023] The petroleum ether is a mixture of pentane and hexane.
[0024] A preparation method of triethyl phosphite, comprising the steps of:
[0025] S1: Preparation of the dropping funnel and flask, sterilize the dropping funnel and flask in a high-temperature steam cabinet, and then dry them before use;
[0026] S2: Preparation of raw materials, respectively put ethanol, phosphorus trichloride, dimethylaniline and petroleum ether in the flasks prepared in S1;
[0027] S3 mixing treatment, the ethanol and dimethylaniline in S2 are placed on the dropping funnel to make ethanol mixed solution, then sherwood oil is imported in the flask containing phosphorus trichloride to make phosphorus trichlorid...
Embodiment 2
[0035] A preparation method of triethyl phosphite, the raw materials are as follows by weight: 4.5 milliliters of ethanol, 1.5 milliliters of phosphorus trichloride, 4.5 milliliters of dimethylaniline, and 18 milliliters of petroleum ether.
[0036] Described ethanol is dehydrated alcohol.
[0037] The petroleum ether is a mixture of pentane and hexane.
[0038] A preparation method of triethyl phosphite, comprising the steps of:
[0039] S1: Preparation of the dropping funnel and flask, sterilize the dropping funnel and flask in a high-temperature steam cabinet, and then dry them before use;
[0040] S2: Preparation of raw materials, respectively put ethanol, phosphorus trichloride, dimethylaniline and petroleum ether in the flasks prepared in S1;
[0041] S3 mixing treatment, the ethanol and dimethylaniline in S2 are placed on the dropping funnel to make ethanol mixed solution, then sherwood oil is imported in the flask containing phosphorus trichloride to make phosphorus ...
Embodiment 3
[0049] A preparation method of triethyl phosphite, the raw materials are as follows by weight: 6 milliliters of ethanol, 2 milliliters of phosphorus trichloride, 6 milliliters of dimethylaniline, and 24 milliliters of petroleum ether.
[0050] Described ethanol is dehydrated alcohol.
[0051] The petroleum ether is a mixture of pentane and hexane.
[0052] A preparation method of triethyl phosphite, comprising the steps of:
[0053] S1: Preparation of the dropping funnel and flask, sterilize the dropping funnel and flask in a high-temperature steam cabinet, and then dry them before use;
[0054] S2: Preparation of raw materials, respectively put ethanol, phosphorus trichloride, dimethylaniline and petroleum ether in the flasks prepared in S1;
[0055] S3 mixing treatment, the ethanol and dimethylaniline in S2 are placed on the dropping funnel to make ethanol mixed solution, then sherwood oil is imported in the flask containing phosphorus trichloride to make phosphorus trichl...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com