augdc precipitation mother liquor recovery and treatment process
A technology of precipitation mother liquor, recovery and treatment, applied in nuclear engineering, radioactive purification, etc., can solve the problems of recovery and treatment process of AUGdC precipitation mother liquor, and achieve the effect of avoiding secondary pollution and reducing consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] AUGdC precipitation mother liquor recovery treatment process, the specific raw materials, equipment and processes used are as follows:
[0025] (1) Raw materials used
[0026] AUGdC precipitation mother liquor; chemically pure nitric acid; chemically pure ammonia water.
[0027] (2) Experimental equipment
[0028] Glass beaker; Buchner funnel; thermometer; infrared heating device; pH meter.
[0029] (3) Process steps
[0030] A. Heating and cooking: Put the AUGdC precipitation mother liquor into a glass beaker, insert the temperature measuring probe to two-thirds of the mother liquor; heat the AUGdC precipitation mother liquor to 100°C with an infrared heating device.
[0031] B. Solid-liquid separation: pour the cooking liquid into the Buchner funnel, and separate the solid and liquid under negative pressure conditions to obtain the filtrate and recover the solid.
[0032] C. Filtrate treatment: add concentrated nitric acid to the filtrate until the pH value is 3, ...
Embodiment 2
[0036] The difference between this embodiment and embodiment 1 is that the process parameters of this embodiment are different, and the specific settings are as follows:
[0037] In step A, heat and cook to 95° C.; in step C, the pH value of the filtrate after acidification is 4; in step D, the adsorption contact time is 40 min.
[0038] It can be seen through testing that the recovery rate of uranium in this embodiment reaches 99.82%, and the recovery rate of gadolinium reaches 94.99%.
Embodiment 3
[0040] The difference between this embodiment and embodiment 1 is that the process parameters of this embodiment are different, and the specific settings are as follows:
[0041] In step A, heat and cook to 105° C.; in step C, the pH value of the filtrate after acidification is 2; in step D, the adsorption contact time is 20 min.
[0042] It can be seen through testing that the recovery rate of uranium in this embodiment reaches 99.84%, and the recovery rate of gadolinium reaches 96.45%.