Coating material for tipping paper
A technology for tipping paper and coating, applied in the field of tobacco, can solve the problems of weak adhesion, unsafe, high solvent residue, and achieve the effects of improving adhesion and reducing toxicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0020] Example: A coating for tipping paper, comprising raw materials of the following components:
[0021] 5-10 parts of iron oxide red powder;
[0022] 5-10 parts of yellow iron oxide powder;
[0023] Acrylic copolymer resin 40-50 parts;
[0024] Styrene-acrylic resin 0.1~0.5 parts;
[0025] 2~3 parts of talcum powder;
[0026] 5~6 parts of polyvinyl butyral;
[0027] 5-10 parts of polyethylene wax;
[0028] 80~100 parts of alcohol solution,
[0029] The components are in parts by weight.
[0030] Among them, the acrylic copolymer resin is a mixture of acrylic copolymer, styrene-acrylic copolymer, self-crosslinking acrylic resin and core-shell acrylic modified resin. In the acrylic copolymer resin, acrylic copolymer accounts for 20%, and styrene-acrylic copolymer It accounts for 30%, self-crosslinking acrylic resin accounts for 20%, and core-shell acrylic modified resin accounts for 30%.
[0031] Iron oxide red powder is 7 parts, iron oxide yellow powder is 7 parts. The alcohol concentrat...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap