A technology for automobile interior decoration and process, which is applied in the field of coating materials for automobile interior decoration and coating technology of automobile interior decoration, can solve the problems of lack of sound insulation effect, poor fire resistance, poor sound insulation effect, etc. The effect of piercing performance, improving flame resistance and sound insulation performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] The coating material includes a soft material layer, a first carbon fiber layer, a sound-insulating PVC composite material layer, a flame-resistant PVC composite material layer, a second carbon fiber layer and a decorative layer from the inside to the outside, wherein the sound-insulating PVC composite material layer is composed of the following Preparation method: provide TiC powder, the particle size of TiC powder is 30 μm; provide chlorosulfonated polyethylene rubber; thinly pass chlorosulfonated polyethylene rubber in a two-roll mill for 5 times; Add TiC powder and knead for 10 minutes to obtain a chlorosulfonated polyethylene rubber / TiC powder blend; put the chlorosulfonated polyethylene rubber / TiC powder blend, PVC particles and processing aids into the internal mixer , and mixed in the internal mixer for 10 minutes to obtain the first mixed material; put the first mixed material into the open mixer, and make the first sheet; put the first sheet into the hot press ...
Embodiment 2
[0024]The coating material includes a soft material layer, a first carbon fiber layer, a sound-insulating PVC composite material layer, a flame-resistant PVC composite material layer, a second carbon fiber layer and a decorative layer from the inside to the outside, wherein the sound-insulating PVC composite material layer is composed of the following Preparation method: provide TiC powder, the particle size of TiC powder is 60 μm; provide chlorosulfonated polyethylene rubber; pass chlorosulfonated polyethylene rubber 10 times in a two-roll mill; Add TiC powder and knead for 20 minutes to obtain a chlorosulfonated polyethylene rubber / TiC powder blend; put the chlorosulfonated polyethylene rubber / TiC powder blend, PVC particles and processing aids into the internal mixer , and mixed in the internal mixer for 20 minutes to obtain the first mixed material; put the first mixed material into the open mixer, and make the first sheet; put the first sheet into the hot press for the fir...
Embodiment 3
[0026] The coating material includes a soft material layer, a first carbon fiber layer, a sound-insulating PVC composite material layer, a flame-resistant PVC composite material layer, a second carbon fiber layer and a decorative layer from the inside to the outside, wherein the sound-insulating PVC composite material layer is composed of the following Preparation method: provide TiC powder, the particle size of TiC powder is 40 μm; provide chlorosulfonated polyethylene rubber; pass chlorosulfonated polyethylene rubber 10 times in a double-roll mill; Add TiC powder and knead for 15 minutes to obtain a chlorosulfonated polyethylene rubber / TiC powder blend; put the chlorosulfonated polyethylene rubber / TiC powder blend, PVC particles and processing aids into an internal mixer , and mixed in the internal mixer for 15 minutes to obtain the first mixed material; put the first mixed material into the open mixer, and make the first sheet; put the first sheet into the hot press for the ...