preparation example Construction
[0019] Such as figure 1 As shown, the preparation method of the carbon black-coal pitch composite spherical activated carbon of the present invention includes the following steps:
[0020] Step a. Soxhlet extraction of medium temperature coal pitch using pyridine solution, after obtaining pitch pyridine solution, add carbon black with a mass ratio of 10% to 50%, and then perform ultrasonic dispersion; add the dispersed pitch pyridine solution to In the suspension solution of polyvinyl alcohol, the mixing mass ratio is 1:1~3, the temperature is raised to 80~90℃, and the temperature is kept for more than 20 minutes, after filtering and drying, the carbon black-coal pitch composite ball is obtained;
[0021] Step b. Place the ceramic boat containing the carbon black-coal pitch composite ball in a tube furnace, and perform the stabilization of the carbon black-coal pitch composite ball in an air atmosphere; the air flow rate is set to 0.3 ~ 0.5L / min; Oxidation heating program: heating ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com