A mosquito tent and deionized water technology, which is applied in the manufacture of rayon, conjugated synthetic polymer rayon, conjugated rayon, etc., can solve the problem of general mosquito repellent effect, drug failure, and inability to achieve long-term mosquito repellent, etc. problem, to achieve a significant effect of repelling mosquitoes, long-term effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] 1. a preparation method of camping mosquito repellent tent, is characterized in that, concrete preparation method is as follows:
[0021] 1) Take 30 parts of deionized water, add 10 parts of absolute ethanol, add 5 parts of sodium silicate and 1 part of polyethylene glycol after mixing, mix and place in a constant temperature water bath for stirring. The temperature of the water bath is 40 ° C. During the stirring process Add 5 parts of ammonium chloride to the mixture, and let it stand for 30 minutes after the stirring is finished;
[0022] 2) After standing still, the obtained milky white precipitate was washed and filtered, then put into a container for heating and drying at 100°C, and the dried powder was used for later use;
[0023] 3) Take 5 parts of alumina, put them into a muffle furnace for high-temperature calcination, rapidly raise the temperature to 500°C, and heat for 6 hours. After the heating is completed, lower the temperature to 400°C, and continue calc...
Embodiment 2
[0030] 1. a preparation method of camping mosquito repellent tent, is characterized in that, concrete preparation method is as follows:
[0031] 1) Take 40 parts of deionized water, add 12 parts of absolute ethanol, add 7 parts of sodium silicate and 2 parts of polyethylene glycol after mixing, mix and place in a constant temperature water bath for stirring. The temperature of the water bath is 45 ° C. During the stirring process Add 3 parts of ammonium chloride to the mixture, and let it stand for 40 minutes after the stirring is finished;
[0032] 2) After standing still, the obtained milky white precipitate was washed and filtered, then put into a container for heating and drying at a heating temperature of 110°C, and the dried powder was used for later use;
[0033] 3) Take 7 parts of alumina, put them into a muffle furnace for high-temperature calcination, quickly raise the temperature to 600°C, and heat for 7 hours. The obtained white powder is taken out for subsequent ...
Embodiment 3
[0040] 1. a preparation method of camping mosquito repellent tent, is characterized in that, concrete preparation method is as follows:
[0041] 1) Take 50 parts of deionized water, add 15 parts of absolute ethanol, add 10 parts of sodium silicate and 3 parts of polyethylene glycol after mixing, mix and place in a constant temperature water bath for stirring. The temperature of the water bath is 50 ° C. During the stirring process Add 5 parts of ammonium chloride to the mixture, and let it stand for 50 minutes after the stirring is finished;
[0042] 2) After standing still, the obtained milky white precipitate was washed and filtered, then put into a container for heating and drying at 120°C, and the dried powder was used for later use;
[0043] 3) Take 10 parts of alumina, put it into a muffle furnace for high-temperature calcination, rapidly raise the temperature to 700°C, and heat for 8 hours. After the heating is completed, lower the temperature to 500°C, and continue cal...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com