A non-toxic dextrin and pigment technology, applied in the field of preparation of low-color-changing dextrin glue for painting pigments, can solve the problems of slow discoloration and affecting product use, and achieve the effects of reducing dosage, inhibiting glue discoloration, and reducing whiteness decline
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0021] A method for preparing dextrin glue with low discoloration for painting pigments, the method comprising the following steps: stirring cornstarch, deionized water, and solid acid evenly, transferring to a frying pan, stirring, cooling down, and sieving to obtain dextrin powder, and separate and recover solid acid; add dextrin powder to polyol, polyamide and deionized water, and cool naturally to obtain the finished product of dextrin glue.
[0022] The specific step of stir-frying is to transfer to a frying pan, raise the temperature to 70° C.-110° C. within 0.1-1.5 hours, and stir-fry for 0.1-3 hours.
[0023] The specific parameters of the heating and stirring are heating to 30-55° C. and stirring for 0.1-1 hour.
[0024] The mass ratio of the uniformly stirred cornstarch, deionized water and solid acid is 100:2-15:0.01-3.
[0025] The mass ratio of the heated and stirred dextrin powder, deionized water, polyol and polyamide is 100:100-800:0.1-15:0.1-5.
[0026] The ...
Embodiment 1
[0040] Get 10kg deionized water, add 250g 300 mesh ZrO to it 2 Load sulfuric acid, mix well, then spray on 200kg cornstarch, stir well. Transfer to a frying pan, heat up to 105°C in 1.5 hours, keep the temperature constant for 4 hours, discharge, cool down, and sieve through a 200-mesh sieve to obtain dextrin powder. Transfer 200kg of dextrin powder to a glue maker, add 400kg of deionized water, 30kg of glycerin, and 1.5kg of polyamide, stir evenly at 50°C, cool naturally, and pack to obtain dextrin glue.
Embodiment 2
[0042] Take 15kg deionized, add 200g 300 mesh ZrO to it 2 Load sulfuric acid, mix well, then spray on 350kg cornstarch, stir well. Transfer to a frying pan, heat up to 105°C in 1.5 hours, keep the temperature for 3 hours, discharge, cool down, and sieve through a 200-mesh sieve to obtain dextrin powder. Transfer 300kg of dextrin powder to a glue maker, add 600kg of water, 60kg of glycerin, and 3kg of polyamide, stir evenly at 45°C, cool naturally, and pack to obtain dextrin glue.