A technology of asphalt mixture and water seepage test, which is applied in the analysis of suspension and porous material, filling slurry, permeability/surface area analysis, etc., which can solve the problems of no water locking function, long-term preservation, poor economy, etc., to achieve High practical value and promotion value, avoid dehydration and drying, reliable sealing effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] This embodiment provides a sealing material for the asphalt mixture water seepage test, which includes 70 parts of waterproof putty, 15 parts of engine oil and 15 parts of diesel oil, and is prepared into required doses according to site requirements. First, add 70 parts of waterproof putty into the mixer, and then add 15 parts of engine oil and 5 parts of diesel oil into the mixer. Stir for 0.5 h at room temperature, take out the stirred mixture, knead the mixture into a ball, and store in a sealed bag. The mixture of engine oil and diesel can form an anti-stick oil film layer between the sealing material and the asphalt mixture pavement or test piece, which can be completely recovered after the sealing test, and the loss rate is less than 1%, and there is no need to repair the asphalt mixture pavement or test piece to clean up. In addition, the waterproof putty itself has anti-corrosion and sealing properties. In the kneaded waterproof putty, it can effectively lock ...
Embodiment 2
[0027] This embodiment provides a sealing material for the asphalt mixture water seepage test, which includes 70 parts of waterproof putty, 20 parts of engine oil and 10 parts of diesel oil, and is prepared into required doses according to site requirements. First, add 70 parts of waterproof putty into the mixer, and then add 20 parts of engine oil and 10 parts of diesel oil into the mixer. Stir for 1 hour at room temperature, take out the stirred mixture, knead the mixture into a ball, and store in a sealed bag.
[0028] To sum up, the present invention utilizes the characteristic of high water absorption rate of the putty material itself, adds an inert oil component material, and after fully mixing with the main material, a microscopic film is formed on the surface of the mixture, so that the moisture inside the mixture is sealed and difficult to volatilize, so it can be kept sealed for a long time Material plasticity. At the same time, the inert oil component material has ...