A production process and stone patch technology, applied in the direction of stone processing equipment, work accessories, manufacturing tools, etc., can solve the problems of easy falling off of decorative tiles and hurting people, saving process and labor costs, not easy to fall off, and beautiful in appearance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0091] The production process of soft thin stone patch includes the following steps:
[0092] S11. smearing cellulose viscose on the template;
[0093] S12. Laying the protective film on the cellulose viscose;
[0094] S13. Leveling;
[0095] S21. Spraying the imitation stone lacquer coating once on the protective film to form a decorative pattern imitation stone varnish layer;
[0096] S22. Secondary spraying of real stone paint on the protective film to form a real stone paint layer;
[0097] S3. Heating and drying the stone-like paint at 30°C with a drying time of 25s;
[0098] S4. Lay fireproof grid cloth on the surface of colorful imitation stone paint, obtain fireproof layer;
[0099] S5. Spray the primer to obtain soft thin stone patch;
[0100] S6. separating the soft thin stone patch from the template;
[0101] S71. Cutting both sides in the width direction;
[0102] S72. Cut to length;
Embodiment 2 Embodiment 7
[0112] Steps S1-S2, S4-S7 are the same as embodiment one, wherein the temperature and time in step S3 are changed:
[0113]
[0114] It can be seen from the above table that when the temperature is 30 and the drying time is 25s, the tear resistance of the soft and thin stone patch is the largest and the service life is the longest. Changing the temperature and drying time will reduce the tear resistance of the soft thin stone material.
[0115] The laying process of soft thin stone patch external wall includes the following steps:
[0116] A1. Apply mud filling on the exterior wall of the building and smooth the wall surface;
[0117] A2. Cut the soft and thin stone patch as needed, and stick the fireproof layer of the soft and thin stone patch on the filling mud;
[0118] A3. Flatten and tear off the protective film.
[0119] In this embodiment, the mud filling is first applied on the outer wall, and glue is mixed in the mud filling, and then the soft thin stone patch is ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com