Metal organic framework material for enhancing combination of chemodynamic therapy and hunger therapy as well as preparation method and application thereof
A technology of metal-organic frameworks and enhanced chemistry, which is applied in the direction of biochemical equipment and methods, organic active ingredients, and medical preparations of non-active ingredients, can solve the problems that are not enough to achieve satisfactory chemical kinetic efficacy, and achieve enhanced chemical kinetics Effect, good development prospects, good biocompatibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Using 2-methylimidazole and zinc nitrate hexahydrate to synthesize ZIF-8 by co-precipitation at room temperature, and wrapping glucose oxidase (GOx) inside MOFs, the specific synthetic route is as follows:
[0037] Dissolve 410mg of 2-methylimidazole in 4mL of ultrapure water, add 1mL of 10mg / mL glucose oxidase ultrapure aqueous solution, and keep stirring, dissolve 37mg of zinc nitrate hexahydrate in 1mL of ultrapure water, drop by drop Add it into the reaction system, react at 25°C for 1 hour, wash the product three times with ultrapure water, centrifuge at 10,000 r / min for 7 minutes, and dry it in a vacuum oven at 37°C for 12 hours to obtain a light yellow powder product. Dissolve 50mg of light yellow powder in 10mL of ultrapure water, add 20μL of 0.15M manganese sulfate monohydrate ultrapure aqueous solution, add 20μL of 0.1M potassium permanganate ultrapure aqueous solution, react for 15min, and wash the product three times with ultrapure water, 10000r / Centrifuge ...
Embodiment 2
[0048] Using 2-methylimidazole, zinc nitrate hexahydrate and copper nitrate hexahydrate to synthesize copper-doped Cu / ZIF-8 by co-precipitation method at room temperature, and wrap glucose oxidase (GOx) inside MOFs, the specific synthesis The route is as follows:
[0049] Dissolve 1.62g of 2-methylimidazole in 20mL of ultrapure water, add 1mL of 25mg / mL glucose oxidase ultrapure aqueous solution, and keep stirring, dissolve 370mg of zinc nitrate hexahydrate and 370mg of copper nitrate hexahydrate in 1mL Add ultrapure water dropwise to the reaction system, stir and react at 25°C for 1h, wash the product with ultrapure water three times, centrifuge at 10000r / min for 7min, and dry in a vacuum oven at 37°C for 12h to obtain a powder product. Dissolve 50mg of light yellow powder in 10mL of ultrapure water, add 20μL of 0.15M manganese sulfate monohydrate ultrapure aqueous solution, add 20μL of 0.1M potassium permanganate ultrapure aqueous solution, react for 15min, and wash the pro...
PUM
Property | Measurement | Unit |
---|---|---|
Size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com