Embodiment 1
[0026] This embodiment is a solid wood furniture panel connector, including a metal connector body and an anti-rust coating compounded on the surface of the metal connector body;
[0027] The solid wood furniture board connector is prepared by the following steps:
[0028] Step 1: Weigh 40 parts of modified styrene-acrylic emulsion, 20 parts of modified diatomaceous earth, 60 parts of deionized water, 2 parts of defoamer, and 3 parts of film-forming aid according to parts by weight;
[0029] Step 2: Add modified styrene-acrylic emulsion, modified diatomaceous earth, and deionized water into the agitator, stir for 2 hours at a speed of 1000r / min, then add defoamer and film-forming aid and continue stirring for 30 minutes , after filtering through a 300-mesh filter screen, the anti-rust coating is obtained;
[0030] Step 3: Apply the anti-rust paint evenly on the surface of the metal connector body, dry for 3 hours at a temperature of 60° C., and wait for the anti-rust paint to...
Embodiment 2
[0042] A solid wood furniture panel connector, comprising a metal connector body and an antirust coating compounded on the surface of the metal connector body;
[0043] The solid wood furniture board connector is prepared by the following steps:
[0044] Step 1: Weigh 50 parts of modified styrene-acrylic emulsion, 25 parts of modified diatomaceous earth, 65 parts of deionized water, 3 parts of defoamer, and 4 parts of film-forming aid according to parts by weight;
[0045] Step 2: Add modified styrene-acrylic emulsion, modified diatomaceous earth, and deionized water into the agitator, stir for 3 hours at a speed of 1500r / min, then add defoamer and film-forming aid and continue stirring for 40 minutes , after filtering through a 300-mesh filter screen, the anti-rust coating is obtained;
[0046] Step 3: Apply the anti-rust paint evenly on the surface of the metal connector body, dry for 4 hours at a temperature of 70° C., and wait for the anti-rust paint to solidify to form a...
Embodiment 3
[0058] This embodiment is a solid wood furniture panel connector, including a metal connector body and an anti-rust coating compounded on the surface of the metal connector body;
[0059] The solid wood furniture board connector is prepared by the following steps:
[0060] Step 1: Weigh 60 parts of modified styrene-acrylic emulsion, 30 parts of modified diatomaceous earth, 70 parts of deionized water, 3 parts of defoamer, and 5 parts of film-forming aid according to parts by weight;
[0061] Step 2: Add modified styrene-acrylic emulsion, modified diatomaceous earth, and deionized water into the agitator, stir for 3 hours at a speed of 2000r / min, then add defoamer and film-forming aid and continue stirring for 50 minutes , after filtering through a 300-mesh filter screen, the anti-rust coating is obtained;
[0062] Step 3: Apply the anti-rust paint evenly on the surface of the metal connector body, dry it for 4 hours at a temperature of 80° C., wait for the anti-rust paint to ...