An anti-condensation and latex paint technology, applied in latex paint, coatings, passive houses, etc., can solve problems such as unsatisfactory performance, inconvenient selection, moldy, etc., to avoid peeling of the coating and reduce indoor energy consumption , Improve the effect of friction resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0033] The preparation method of the anti-condensation heat preservation latex paint of the present invention specifically comprises the following steps:
[0034] Step 1: Add water into a container and start stirring, add bentonite;
[0035] Step 2: After the solution is uniform and thickened, add multifunctional additives, dispersants, defoamers, antibacterial agents and stir evenly;
[0036] Step 3: Mix titanium dioxide, mica powder, and heavy calcium, and disperse evenly;
[0037] Step 4: Add pure acrylic emulsion and silicone resin emulsion and mix well;
[0038] Step 5: Add insulation material and mix well;
[0039] Step 6: Add film-forming aids, antifreeze agents, and water repellents and stir evenly to obtain the finished anti-condensation and thermal insulation latex paint.
[0040] The heat insulating material is prepared as follows: uniformly mixing microbeads, nano silicon dioxide and airgel slurry in proportion to obtain the heat insulating material.
Embodiment 1
[0042] In parts by weight, the anti-condensation heat preservation latex paint in the present embodiment consists of the following components:
[0043] 28.9 parts of water, 0.3 parts of bentonite, 0.2 parts of multifunctional additives, 0.3 parts of dispersant, 0.3 parts of defoamer, 1 part of antibacterial agent, 5 parts of titanium dioxide, 4 parts of mica powder, 10 parts of heavy calcium, airgel paste 4 parts of materials, 5 parts of ceramic hollow microspheres, 5 parts of nano-silica, 22 parts of pure acrylic emulsion, 10 parts of silicone resin emulsion, 0.5 parts of film-forming aids, 0.5 parts of antifreeze, and 3 parts of waterproofing agent.
Embodiment 2
[0045] In parts by weight, the anti-condensation heat preservation latex paint in the present embodiment consists of the following components:
[0046] 32.3 parts of water, 0.4 parts of bentonite, 0.3 parts of multifunctional additives, 0.5 parts of dispersant, 0.5 parts of defoamer, 2 parts of antibacterial agent, 3 parts of titanium dioxide, 3 parts of mica powder, 5 parts of heavy calcium, airgel slurry 3 parts of materials, 6 parts of ceramic hollow microspheres, 6 parts of nano-silica, 20 parts of pure acrylic emulsion, 10 parts of silicone resin emulsion, 1.5 parts of film-forming aid, 1.5 parts of antifreeze, and 5 parts of waterproofing agent.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle diameter | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 