Embodiment 1
[0030] (1) will be the polyvinyl alcohol 8kg of PVA17-88, boric acid 0.1kg, pure water 65kg, antibacterial agent composition 0.3kg (the composition of nano silver and nano zinc oxide with mass ratio 1:5), antifungal combination 1.5kg of substance (sodium diacetate and octanoyl hydroxamic acid are combined in a mass ratio of 1:1), 0.05kg of lavender essential oil are stirred and mixed to obtain functional liquid for subsequent use;
[0031] (2) 15kg of dimethicone, 3kg of emulsifier (sodium tetrapropylene alkyl benzene sulfonate, emulsifier T-80, emulsifier OP-10 are compounded according to the mass ratio of 1:2:4) were added to the high shear Cut the emulsification and disperser, disperse at 1000 rpm for 3 minutes; then add 60kg of pure water to the high shear emulsification and disperser, after adding water, increase the speed of the high shear emulsification and disperser to 3000 rpm, and treat for 5 minutes to obtain the emulsified base liquid backup;
[0032] (3) The func...
Embodiment 2
[0034] (1) the polyvinyl alcohol 8kg, boric acid 0.1kg, pure water 65kg, antibacterial agent composition 0.3kg (nano-silver and polyhexamethylene biguanide hydrochloride with mass ratio 1:5) of PVA17-88 material), mildew-proof composition 1.5kg (sodium diacetate and octanoyl hydroxamic acid are combined in a mass ratio of 1:1), 0.05kg of lavender essential oil are stirred and mixed to obtain functional liquid for subsequent use;
[0035] (2) 15kg of dimethicone, 3kg of emulsifier (sodium tetrapropylene alkyl benzene sulfonate, emulsifier T-80, emulsifier OP-10 are compounded according to the mass ratio of 1:2:4) were added to the high shear Cut the emulsification and disperser, disperse at 1000 rpm for 3 minutes; then add 60kg of pure water to the high shear emulsification and disperser, after adding water, increase the speed of the high shear emulsification and disperser to 3000 rpm, and treat for 5 minutes to obtain the emulsified base liquid backup;
[0036] (3) The functi...