Preparation method of coconut oil fiber membrane cloth
A coconut fiber and fiber film technology, applied in chemical instruments and methods, liquid/gas/steam fiber/sliver/roving treatment, non-woven fabrics, etc., to achieve the effect of non-polluting and wide-ranging sources
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A preparation method of coconut oil fiber membrane cloth, comprising the following steps:
[0028] Step 1, prepare plant fiber, 10% coconut fiber, 20% seaweed fiber, 30% cotton and linen fiber and 40% cotton fiber;
[0029] Step 2: Mix coconut fiber, seaweed fiber, cotton hemp fiber and cotton fiber. After fully mixing, pour each component into a fiber softener for soaking and softening, and control the softening temperature to 20°C and soak time to 24 h. ;
[0030] Step 3: After the softening is completed, the fibers are cleaned and then dried, and impurities and short fibers are removed to obtain dry mixed fibers and carding;
[0031] Step 4, before the spunlace processing, firstly, the mixed fibers are subjected to humidification treatment, and then subjected to spunlace processing, and then after finishing, drying and winding to obtain the coconut oil fiber membrane cloth.
Embodiment 2
[0033] A preparation method of coconut oil fiber membrane cloth, comprising the following steps:
[0034] Step 1, prepare plant fiber, plant fiber is coconut fiber 15%, seaweed fiber 20%, cotton and linen fiber 15% and cotton fiber 50%;
[0035] Step 2, mix coconut fiber, seaweed fiber, cotton hemp fiber and cotton fiber, pour each component into a fiber softener for soaking and softening after fully mixing, and control the softening temperature to be 35°C, and the soaking time to be 30h;
[0036] Step 3: After the softening is completed, the fibers are cleaned and then dried, and impurities and short fibers are removed to obtain dry mixed fibers and carding;
[0037] Step 4, before the spunlace processing, firstly, the mixed fibers are subjected to humidification treatment, and then subjected to spunlace processing, and then after finishing, drying and winding to obtain the coconut oil fiber membrane cloth.
Embodiment 3
[0039] A preparation method of coconut oil fiber membrane cloth, comprising the following steps:
[0040] Step 1, prepare plant fiber, plant fiber is coconut fiber 55%, seaweed fiber 25%, cotton fiber 10% and cotton fiber 10%;
[0041] Step 2: Mix coconut fiber, seaweed fiber, cotton hemp fiber and cotton fiber, pour each component into a fiber softener for soaking and softening after fully mixing, and control the softening temperature to be 55°C and soaking time to be 25h;
[0042] Step 3: After the softening is completed, the fibers are cleaned and then dried, and impurities and short fibers are removed to obtain dry mixed fibers and carding;
[0043] Step 4, before the spunlace processing, firstly, the mixed fibers are subjected to humidification treatment, and then subjected to spunlace processing, and then after finishing, drying and winding to obtain the coconut oil fiber membrane cloth.
PUM
| Property | Measurement | Unit |
|---|---|---|
| pore size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More