Printing plate material of containing agent for increasing acid available for computer to carry out plate making directly
A proliferating agent and computer technology, applied in the field of heat-crosslinked computer-to-plate-making plates, can solve the problems of less than 150 sets installed, incomplete resin cross-linking, plate thickness thinning, etc., to improve differential solubility , shorten the post-baking time, reduce the effect of post-baking temperature
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] Weigh soluble phenolic resin, m-cresol resin, latent Bronsted acid salt, and terephthalaldehyde and dissolve them in acetone respectively, and prepare a solution with a certain concentration for later use. The infrared dye was weighed and dissolved in 1-methoxy-2-propanol, and the acid multiplier 1,4-bis(p-toluenesulfonyloxy)cyclohexane was dissolved in dichloromethane, and set aside. The specific preparation process is as follows:
[0031] (1) measure the acetone solution of 10ml 30% resol resin;
[0032] (2) measure the acetone solution of the m-cresol resin of 10ml 30%;
[0033] (3) Take 2.0g iodonium salt and dissolve it in 2ml acetone;
[0034] (4) Take by weighing 1.0g terephthalaldehyde and be dissolved in 2ml acetone;
[0035] (5) Weigh 0.5g infrared absorbing dye and dissolve it in 10ml 1-methoxy-2-propanol solution;
[0036] (6) Weigh 0.5 g of di-p-toluenesulfonic acid-1,4-cyclohexanediester and dissolve it in 2 ml of dichloromethane.
[0037] After the a...
Embodiment 2
[0040] According to the method of Example 1, when configuring the photosensitive solution, use 0.5g ketal compound T 1
[0041]
[0042]Instead of di-p-toluenesulfonic acid-1,4-cyclohexanediester, the solid content of the acid proliferator is 5%. After exposure, post-baking and development, a negative thermal crosslinking computer-to-plate plate material that can be used for printing is obtained. .
Embodiment 3
[0044] According to the method of Example 1, when configuring the photosensitive solution, use 0.5g benzylsulfonate compound T 2
[0045]
[0046] Instead of di-p-toluenesulfonic acid-1,4-cyclohexanediester, the solid content of the acid proliferator is 5%. After exposure, post-baking and development, a negative thermal crosslinking computer-to-plate plate material that can be used for printing is obtained. .