Manufacturing method of washable mulberry silk quilt
A manufacturing method and technology of silk cotton quilts, which are applied in the field of manufacturing washable mulberry silk cotton quilts, can solve the problems of reduced air permeability and warmth retention, failure to recover fluffy, and reduced bulkiness, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0023] Spray silkworm cocoons with 65°C sodium hydroxide solution, and the silk will gradually separate from the cocoon layer. Use a machine for making cotton sheets to make cotton sheets from the cocoons, and place them at room temperature for 2 days to make the cotton sheets expand again, and put them in water at 100°C And add sodium hydroxide, mercerized soap, sodium hydroxide and cook to make the cotton sheet degummed, rinse it, cool and dehydrate it, add glacial acetic acid, silicone epoxy derivatives, and mercerized softener, filter the water again, and put it on the silk cotton Add organic fluorine resin softener and cross-linking agent containing polyacrylate structure to the sheet, then dry the treated cotton sheet at 110°C for 45 minutes, manually stretch the cotton sheet to a fluffy state, press The size requires cutting the cotton tire, putting it into a quilt cover, and packaging the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com