a laminated film, easy peeling technology, applied in the direction of film/foil adhesives, synthetic resin layered products, transportation and packaging, etc., can solve the problems of easy peeling, easy breakage of surface materials, inferior water resistance, etc., to achieve easy peeling and laminate

Inactive Publication Date: 2003-08-14
YUPO CORP
View PDF2 Cites 29 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Benefits of technology

0057] [Formation of Pressure-Sensitive Adhesive Layer]
0058] A pressure-sensitive adhesive layer can be provided on the side of the peelable surface layer (B) opposite to the base layer (A) of the easily peelable laminated film (i) of the invention (i.e., next to the peelable surface layer or next to the protective layer, if provided), if desired.
0059] By providing a pressure-sensitive adhesive layer on an easily peelable laminated film, an easily peelable laminated label (ii) can be obtained.
0060] As such pressure-sensitive adhesives, rubber-based pressure-sensitive adhesives, acryl-based pressure-sensitive adhesives and silicon-based pressure-sensitive adhesives are representative. Specific examples of rubber-based pressure-sensitive adhesives include polyisobutylene rubber, butyl rubber and mixtures thereof, and pressure-sensitive adhesives obtained by blending these rubber-based pressure-sensitive adhesives with a tackifier, e.g., abietic acid rosin ester, a terpene-phenol copolymer, or a terpene-indene copolymer. Specific examples of acryl-based pressure-sensitive adhesives include those having a glass transition temperature of -20.degree. C. or less, e.g., a 2 thylhexyl acrylate-n-butyl acrylate copolymer and a 2-ethylhexyl acrylate-ethyl acrylate-methyl methacrylate copolymer.
0061] As the types of these pressure-sensitive adhesives, a solvent-type, an emulsion-type and a hot melt-type are used. In general, a pressure-sensitive adhesive layer is laminated by coating a solvent-type or emulsion-type adhesive.
0062] Coating is performed by means of a roll coater, a blade coater, a bar coater, an air knife coater, a gravure coater, a reverse coater, a die coater, a lip coater, a spray coater, or a comma coater and, if necessary, smoothing is performed, and a pressure-sensitive adhesive layer is formed through drying.

Problems solved by technology

There has been conventionally such a problem in the salesroom of foods in supermarkets and department stores that there are persons who peel off the pressure-sensitive adhesive price label of lowered price from the foods on sale nearing eatable limit and replace this price label with the price label of foods of normal price and purchase the foods at a cheaper price.
However, there are problems that these labels for preventing re-pasting are expensive, an adhesive remains on the peeled surface and sticky to the touch, or dusts are adhered on the surface.
However, this method is not only complicated but also inferior in water resistance when paper made of pulp is used as the surface material of the first layer, so that the surface material is easily broken and peeled off from the material adhered when it is brought into contact with water.
Therefore, this label is not suited to be a label for a sealed vessel containing water, e.g., pickles, tofu (bean curd), konjak (devil's tongue), etc.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

example 1

[0084] After each of thermoplastic resin composition d as layer (B), thermoplastic resin composition b as layer (A1), and thermoplastic resin composition c as layer (A2) was kneaded in each extruder set at 230.degree. C., they were supplied to a co-extrusion die set at 250.degree. C., laminated in the die and extruded in a sheet. The laminate was cooled by a cooler, thereby a three-layer unstretched sheet was obtained. The unstretched sheet was heated at 130.degree. C. and stretched 5 times in the machine direction.

[0085] The above sheet was cooled to a temperature of 60.degree. C., again heated to a temperature of 150.degree. C. and stretched 8.0 times in the transverse direction in a tenter oven, subjected to annealing treatment at a temperature of 162.degree. C., cooling at 60.degree. C., and corona discharge treatment, and then trimming, thereby a laminated film of a three-layer structure [(B) / (A1) / (A2): 1 / 49 / 10 .mu.m in thickness, stretched layer constitution: biaxial / biaxial / b...

example 2

[0086] After each of thermoplastic resin composition d as layer (B) and thermoplastic resin composition b as layer (A1) was kneaded in each extruder set at 230.degree. C., they were supplied to a co-extrusion die set at 250.degree. C., laminated in the die and extruded in a sheet. The laminate was cooled by a cooler, thereby a two-layer unstretched sheet was obtained. The unstretched sheet was heated at 130.degree. C. and stretched 4 times in the machine direction.

[0087] Thermoplastic resin composition b as layer (A2) was kneaded in an extruder set at 250.degree. C. and extruded in a sheet, and this sheet was laminated on the above-prepared 4 time-stretched film (A1), thereby a three-layer structure laminated film was obtained. The three-layer structure laminated film was cooled to a temperature of 60.degree. C., again heated to about 160.degree. C. by a tenter oven and stretched 7.5 times in the transverse direction, subjected to annealing treatment in a heat-set zone adjusted to 1...

example 3

[0088] After each of thermoplastic resin composition f as layer (B), thermoplastic resin composition b as layer (A1), and thermoplastic resin composition c as layer (A2) was kneaded in each extruder set at 240.degree. C., they were supplied to a co-extrusion die set at 270.degree. C., laminated in the die and extruded in a sheet. The laminate was cooled by a cooler, thereby a three-layer unstretched sheet was obtained. The unstretched sheet was heated at 120.degree. C. and stretched 5 times in the machine direction, subjected to annealing treatment at 160.degree. C., corona discharge treatment, and then trimming, thereby a laminated film of a three-layer structure [(B) / (A1) / (A2): 4 / 46 / 10 .mu.m in thickness, stretched layer constitution: monoaxial / monoaxial / monoaxial] having a thickness of 60 .mu.m, a peeling strength of 90 g / cm, and an opaqueness of 87% was obtained.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
thicknessaaaaaaaaaa
particle diameteraaaaaaaaaa
Login to view more

Abstract

An easily peelable laminated film includes a laminate of a peelable surface layer (B) having a peeling strength of 5 to 100 g/cm with a base layer (A) containing a thermoplastic resin. The laminated film of the invention provides an easily peelable laminated film excellent in water resistance as a base materialfor, for example, concealing seals and labels for preventing re-pasting. The easily peelable laminated film of the invention requires no specific process to start peeling.

Description

[0001] The present invention relates to an easily peelable laminated film comprising a laminate of a base layer (A) comprising a thermoplastic resin, and a peelable surface layer (B) weaker in strength than the base layer (A).[0002] An easily peelable laminated film is useful as a base material of, for example, delivery slips, concealing seals of post cards and passbooks, labels for preventing re-pasting, seals for preventing alteration, application seals, and coupons free of remaining adhesives.[0003] There has been conventionally such a problem in the salesroom of foods in supermarkets and department stores that there are persons who peel off the pressure-sensitive adhesive price label of lowered price from the foods on sale nearing eatable limit and replace this price label with the price label of foods of normal price and purchase the foods at a cheaper price.[0004] Therefore, a label for preventing re-pasting which is easily known to be the peeled label after peeling and re-pas...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(United States)
IPC IPC(8): B32B3/26B32B7/06B32B27/20B32B27/32C09J7/40
CPCB32B3/26Y10T428/1462B32B27/20B32B27/32C09J7/0225Y10T428/1476Y10T428/1486Y10T428/24372Y10T428/1471Y10T428/14Y10T428/1405Y10T428/1452Y10T428/24876Y10T428/24851B32B7/06C09J7/40
Inventor KOIKE, HIROSHI
Owner YUPO CORP
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products