Process for refining high-purity yellow phosphorus
A production method and yellow phosphorus technology, applied in chemical instruments and methods, phosphorus compounds, inorganic chemistry, etc., can solve the problems of complex production links, harsh requirements, poor safety, etc., and achieve high arsenic removal rate and impurity removal rate. , easy operation, low cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0011] Embodiment: 20% by weight of industrial yellow phosphorus is put into a refined pot filled with 80% by weight of pure water with interlayer insulation, heated to 50° C., and melted into liquid yellow phosphorus. Add carbonate with a weight of 12% of the weight of industrial yellow phosphorus into the liquid yellow phosphorus. It can be ammonium bicarbonate or ammonium bicarbonate. After heating to 75°C, use a stirrer with a speed of 70 to 100 rpm to stir and react for 2 hours. , and then washed twice with pure water at 80°C, and allowed to settle for 1 hour.
[0012] The above-mentioned treated liquid yellow phosphorus is put into the interlayer insulation of the reducing agent solution prepared by the nitric acid solution with a concentration of 17%, a weight of 180% of the industrial yellow phosphorus weight and a concentration of 8%, and a weight of 20% of the industrial yellow phosphorus weight. In the enamel refining pot, heat to 75°C, use a stirrer with a speed of...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com