Cleaning antirust agent and preparation method thereof
A technology of rust inhibitor and bactericide, applied in the field of cleaning rust inhibitor and its preparation, can solve the problems of long time for cleaning parts, inability to use high-pressure equipment, no rust resistance, etc., and achieves a simple and scientific mechanism of action and a simple cleaning process. The effect of inhibiting the formation of bacteria
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] Each component and its content, weight ratio are respectively:
[0034] Ethylenediaminetetraacetic acid solution: content 50% ratio 1.5%
[0035] Triethanolamine solution: content 99% ratio 3.5%
[0036] Monoethanolamine solution: content 99% ratio 1%
[0037] Synthetic borate ester solution: content 70% ratio 5%
[0038] Polyacrylic acid solution: content 30% ratio 7%
[0039] Triazine fungicide solution: content 90% ratio 1%
[0040] Water: Proportion 81%.
[0041] The preparation method is as follows:
[0042] (1). Add 50% of the proportioned water into the reactor A, heat up to 40°C, then add ethylenediaminetetraacetic acid solution, triethanolamine solution and monoethanolamine solution according to the proportioning ratio to react, at a temperature of 40°C Keep warm for four hours to form a water-based antirust agent;
[0043] (2). Add another 50% of water to the reaction kettle B, and add polyacrylic acid solution according to the ratio under stirring cond...
Embodiment 2
[0047] Each component and its content, weight ratio are respectively:
[0048] Ethylenediaminetetraacetic acid solution: content 65% ratio 1.2%
[0049] Triethanolamine solution: content 99% ratio 3.8%
[0050] Monoethanolamine solution: content 99% ratio 0.6%
[0051] Synthetic boric acid ester solution: content 70% ratio 7.4%
[0052] Polyacrylic acid solution: content 30% ratio 8%
[0053] Triazine fungicide solution: content 90% ratio 2%
[0054] Water: Proportion 77%.
[0055] The preparation method is as follows:
[0056] (1). Add 50% of the proportioned water into the reactor A, heat up to 38°C, then add ethylenediaminetetraacetic acid solution, triethanolamine solution and monoethanolamine solution according to the proportion to react, and the temperature is 42°C. Keep warm for four hours to form a water-based antirust agent;
[0057] (2). Add another 50% of water to the reactor B, and add the polyacrylic acid solution according to the proportion under stirring ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com