The invention relates to the technical field of
solid waste recovery, and provides a method for efficiently, simply and conveniently recovering
asphalt based on a small amount of
asphalt mixture, which comprises the following steps: S1, taking an
asphalt mixture sample, adding water, and carrying out ultrasonic cleaning to remove impurities on the surface of the sample; s2, putting the
impurity-removed and dried sample into a mixed
solvent, and soaking for 20-40 minutes until the surface of the aggregate is not coated with asphalt; the mixed
solvent is prepared from 1, 1-diethoxyethane and methyl tert-butyl
ether; and S3, carrying out reduced pressure suction
filtration and
centrifugation on the mixture obtained in the step S2, placing the supernatant in a fuming
cupboard for preliminary volatilization, and then placing the supernatant in a
forced air drying oven for
solvent evaporation at 60-105 DEG C to obtain the recycled asphalt. According to the method, the low-boiling-point solvent 1, 1-diethoxyethane and methyl tert-butyl
ether are compounded, and subsequent reduced-pressure suction
filtration,
centrifugation and volatilization treatment are combined, so that the method for efficiently, simply and conveniently recovering the asphalt from the asphalt mixture is realized, and compared with an existing Ambusan method and a
rotary evaporator method, the method has the advantages that the recovered asphalt is high in fidelity, and the
recovery rate is high. And no
organic solvent is left.