Special modified cold-mixing asphalt for cold-region normal-temperature mixing-type asphalt concrete

A technology of asphalt concrete and cold-mixed asphalt, which is applied to building insulation materials, building components, buildings, etc., can solve the problems of cold-mixed asphalt demulsification speed, poor adaptability to regions, and short storage time, so as to improve the softening point, Effects of reduced kinematic viscosity and long storability

Inactive Publication Date: 2010-06-16
李国涛
View PDF2 Cites 9 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0007] The purpose of the present invention is to provide a special modified cold-mix asphalt for normal-temperature mixing asphalt concrete in cold regions, which is used to replace hot asphalt or heat-modified asphalt, and solve the problem of too fast demulsification of cold-mix asphalt, unstable performance, and storage problems. Short time and poor adaptation to regional issues

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0025] Example 1: Preparation of cold-mix asphalt used in cold regions

[0026] Components: by weight percentage, heavy traffic asphalt: 70%, linear liquid SBS: 5%, cationic surfactant (as above): 10%, organic additives (as above): 4%, water: 11%.

[0027] Preparation method: heat asphalt to 170°C; heat water to 45°C, mix with cationic surfactant and grind to form soap liquid; mix 70% asphalt with 21% soap liquid and 5% liquid linear modifier and 4% organic additives are mixed in the blender, quickly ground, stored in the transition tank and stirred for 60 minutes, poured into the finished product tank and cooled to room temperature.

Embodiment 2

[0028] Example 2: Preparation of cold-mix asphalt used in cold regions

[0029] Components: by weight percentage, heavy traffic asphalt: 60%, linear liquid SBS: 5%, cationic surfactant: 10%, organic auxiliary agent: 4%, water: 21%.

[0030] Preparation method: heat the asphalt to 130°C, and heat the soap liquid to 65°C. After mixing 60% bitumen, 31% soap liquid and 5% linear liquid modifier in the blender, form a stable suspension by grinding, stir in the transition tank for 60 minutes, and store it in the finished product tank , cooled to room temperature.

Embodiment 3

[0031] Example 3: Preparation of cold-mix asphalt used in cold regions

[0032] Components: by weight percentage, heavy traffic asphalt: 50%, linear liquid SBS: 5%, cationic surfactant: 10%, organic auxiliary agent: 4%, water: 31%.

[0033] Preparation method: heat the asphalt to 100°C, and heat the soap liquid to 50°C. Add 50% asphalt, 41% soap liquid and 5% linear liquid modifier into the blender at the same time, grind it into the transition tank, stir for 60 minutes, enter the finished product tank and cool to room temperature.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
softening pointaaaaaaaaaa
Login to view more

Abstract

The invention provides special modified cold-mixing asphalt for cold-region normal-temperature mixing-type asphalt concrete, which comprises linear liquid SBS, heavy traffic asphalt, surfactant, organic additives and water. The weight percentages of the components are: 50 to 70 percent of heavy traffic asphalt, 2.5 to 15 percent of linear liquid SBS, 1.2 to 11 percent of cationic surfactant, 3 to 6 percent of organic additives, and 20 to 30 percent of water. The water and the cationic surfactant are mixed pro rata and then are fully mixed through an emulsifier to form soap liquid; the heavy traffic asphalt is heated to between 100 and 170 DEG C; the soap liquid is heated to between 45 and 80 DEG C; the heavy traffic asphalt, the soap liquid, the linear liquid SBS and the organic additives are rapidly mixed in a mixing-melting device; and a uniform stable suspended substance is formed through a grinding machine, fully stirred, cooled to normal temperature and stored, thus the asphalt can be obtained. The problem that cold-mixing asphalt is too fast to demulsify, unstable in performance, short in storage time and poor in regional adaptability is solved. Evaporation residue of the asphalt mixture can greatly improve pavement performance. In addition, the asphalt has the advantages of simple process, stable performance and wide use.

Description

technical field [0001] The invention relates to a cold-mix asphalt for highway pavement, in particular to a modified cold-mix asphalt specially used for normal-temperature mixing asphalt concrete in cold regions. Background technique [0002] A large number of asphalt is used as the pavement cementitious material for highway pavement. As a cementitious material, asphalt must first be heated and melted, and the high-grade pavement must be modified and processed. At the same time, the aggregate must be heated to 200°C, and then mixed. Under heat preservation, it will be transported, paved, and rolled to form asphalt pavement. All processes consume a lot of fuel and generate greenhouse gases. At the same time, the project construction is seriously affected by the climate, the process coordination requirements are strict, the material utilization rate is low, and the waste is serious. Seriously pollute the environment and the health of construction workers. [0003] Chinese ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C08L95/00C08L53/02C08K5/20C08K5/3445C08K5/17C08K5/10C04B26/26
Inventor 李国涛
Owner 李国涛
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products