A water-based polyurethane and cationic technology, applied in the direction of water-repellent addition, coating, paper coating, etc., can solve the problems of large odor of emulsion, long synthesis time, complicated process, etc., achieve good water resistance and stability, and improve performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Example 1: Under the operating conditions of the comparative example, add 1.0 g of hydroxypropyl polydimethylsiloxane (8427) to the three-necked flask before vacuumizing, and finally add 53.79 g of water to obtain a theoretical solid content of 30%. , Pale yellow translucent emulsion.
Embodiment 2
[0027] Example 2: Under the operating conditions of the comparative example, add 0.5 g of glyceryl monostearate to the three-necked flask before vacuumizing, and finally add 44.53 g of water to obtain a milky white translucent emulsion with a theoretical solid content of 35%.
Embodiment 3
[0028] Embodiment 3: under the operating condition of embodiment 1, change 5.68gTDI into 7.25g IPDI, add 0.1mol / L dilute hydrochloric acid 1.28g (neutralization degree is 80%) when neutralizing, add 225.05g water at last, get Theoretical solid content is 10%, colorless translucent emulsion.