Embodiment 1
[0014] 30-60 g / m² natural colored silk. The concentration of the degumming solution is 15g / l sodium hydroxide, 5g / l sodium tetraborate, and 15g / l Remibond A. After soaking or padding the silk fabric, put it in cold storage at 20°C for 24 hours, and then wash it with water. Auxiliaries and hydrolyzed sericin on silk fabrics are washed and finally dried.
Embodiment 2
[0016] 30-60 g / m² natural colored silk. The concentration of the degumming solution is potassium hydroxide 15g / l, sodium tetraborate 5g / l, and Remibond A 15g / l. After soaking or padding the silk fabric, put it in a cold stack at 30°C for 16 hours, then wash it with water, and absorb it on Auxiliaries and hydrolyzed sericin on silk fabrics are washed and finally dried.
Embodiment 3
[0018] 30-60 g / m² natural colored silk. The concentration of the degumming solution is sodium hydroxide 15g / l, sodium tetraborate 5g / l, and Remibang A 15g / l. After soaking or padding the silk fabric, put it in cold storage at 40°C for 10 hours, and then wash it with water. Auxiliaries and hydrolyzed sericin on silk fabrics are washed and finally dried.