Stabilizer composition for polyamide
A composition, polymer technology, applied in polyamide coatings, devices for coating liquids on surfaces, coatings, etc., can solve problems such as error reports and failures
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0035] figure 1 Shown is a metal lead frame 10 which is injection encapsulated with one embodiment of a polymer composition according to the invention and subsequently stored in oil at a constant temperature of 150° C. for about 1700 hours. The polymer composition here comprises polyamide PA66, 35% by weight of glass fibers, 0.1% by weight of copper(I) iodide and 1% by weight of potassium iodide.
[0036] figure 2 Shown is a metal lead frame 20 which is injection encapsulated with a conventional amine stabilized polyamide polymer composition and subsequently stored in oil at a constant temperature of 150°C for about 1700 hours.
[0037] like figure 1 and 2 shown, with figure 2 Different from the section 21 of the lead frame 20 shown in the conventional injection molding package, figure 1 The section 11 of the leadframe 10 injection-molded according to the invention shown in , forms significantly less conductive deposits.