Compound foaming agent for foam concrete and preparation method thereof

A foam concrete and foaming agent technology, applied in the field of building materials, can solve the problems of easy combustion, less functions, high bulk density, etc., and achieve the effect of excellent foaming performance, long stable time, and high foaming ratio

Inactive Publication Date: 2013-01-23
TONGJI UNIV
View PDF2 Cites 26 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

These types of thermal insulation materials have their own advantages and disadvantages: 1) Organic thermal insulation materials have the advantages of good thermal insulation performance, strong processability and good compactness, but have disadvantages such as easy deformation, poor durability and easy combustion; 2) Inorganic thermal insulation materials have the advantages of good fire resistance, stable performance and good durability, but there are disadvantages such as slightly higher bulk density and poor thermal insulation effect; 3) Composite thermal insulation materials have good thermal insulation performance, small deformation coefficient, It is an ideal thermal insulation material with a series of advantages such as wide source of raw materials and the ability to absorb waste.
At present, domestic foaming agents generally have less functions and poor stability, so that the strength of the prepared foamed concrete products is poor. Therefore, the research on composite foaming agents is the key to preparing foamed concrete with excellent performance.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0035] Embodiment 1, a composite foaming agent for foamed concrete and its preparation method, the foaming agent according to surfactant 100, protein foaming agent 0.1, foam stabilizer 0.1, coagulant 10, water reducing agent 10 Formulated with a weight ratio. The preparation method is to first prepare a surfactant solution with a mass concentration of 0.6%, and dissolve lauroyl diethanolamine in water at 50°C-60°C to prepare a solution with a mass solubility of 10%, and then sequentially dissolve the lauryl diethanolamine according to the above weight ratio Protein foaming agent, lauroyl diethanolamine solution, coagulant and water reducing agent are mixed into the surfactant solution, and finally stirred evenly. The foaming ratio of this foaming agent is 35, the subsidence distance is 12mm in 1h, and the bleeding volume in 1h is 70ml.

Embodiment 2

[0036] Embodiment 2, a composite foaming agent for foamed concrete and its preparation method, the foaming agent according to surfactant 100, protein foaming agent 1, foam stabilizer 0.5, coagulant 20, water reducer 30 Formulated with a weight ratio. The preparation method is to first prepare a surfactant solution with a mass concentration of 0.6%, and dissolve lauroyl diethanolamine in water at 50°C-60°C to prepare a solution with a mass solubility of 10%, and then sequentially dissolve the lauryl diethanolamine according to the above weight ratio Protein foaming agent, lauroyl diethanolamine solution, coagulant and water reducing agent are mixed into the surfactant solution, and finally stirred evenly. The foaming ratio of this foaming agent is 46, the subsidence distance is 8mm in 1h, and the bleeding volume in 1h is 60ml.

Embodiment 3

[0037] Embodiment 3, a composite foaming agent for foamed concrete and its preparation method, the foaming agent according to surfactant 100, protein foaming agent 5, foam stabilizer 3, coagulant 50, water reducing agent 70 Formulated with a weight ratio. The preparation method is to first prepare a surfactant solution with a mass concentration of 0.6%, and dissolve lauroyl diethanolamine in water at 50°C-60°C to prepare a solution with a mass solubility of 10%, and then sequentially dissolve the lauryl diethanolamine according to the above weight ratio Protein foaming agent, lauroyldiethanolamine solution, coagulant and water reducing agent are mixed into the surfactant solution, and then stirred evenly. The foaming ratio of this foaming agent is 50, the subsidence distance is 7mm in 1h, and the bleeding volume in 1h is 40ml.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention belongs to the technical field of building materials, and specifically relates to a compound foaming agent for a foam concrete and the preparation method of the compound foaming agent. The compound foaming agent is composed of a surfactant, a protein foaming agent, a foam stabilizing agent, a coagulation accelerator and a water reducing agent. The compound foaming agent provided by the invention is doped with few protein foaming agent and foam stabilizing agent in a surfactant solution to remarkably improve the foaming capability and the foam stabilizing time of the surfactant solution and create favorable conditions for preparing the foam concrete at a low-density grade (not more than 500 Kg/m<3>). In addition, the coagulation accelerator is doped to accelerate the condensation of cement slurry and effectively prevent collapsing; the water reducing agent is doped to improve the working property of a freshly mixed concrete, and reduce the water dosage and improve the strength of the foam concrete at the same time. The product provided by the invention has various functions, and is not limited to only prepare the foam; at the same time, the product provided by the invention has the actions of accelerating coagulation and reducing water, and the product provided by the invention is suitable for preparing the low-density foam concrete.

Description

technical field [0001] The invention belongs to the technical field of building materials, and in particular relates to a composite foaming agent for foam concrete and a preparation method thereof. Background technique [0002] Since my country began to implement building thermal insulation and energy-saving projects in 2005, thermal insulation materials have developed rapidly. At present, common insulation materials are mainly divided into organic insulation materials, inorganic insulation materials and composite insulation materials. Among them, organic thermal insulation materials include expanded polystyrene, extruded polystyrene, foamed polyurethane and expanded polystyrene particles, etc., and inorganic thermal insulation materials include expanded perlite, closed-cell perlite, expanded vermiculite, hollow vitrified microspheres and Rock wool (asbestos), etc., and composite thermal insulation materials are a type of material that is processed and produced by combining...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C04B24/20C04B24/28
Inventor 孙振平刘警
Owner TONGJI UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products