The invention relates to lightweight
thermal insulation concrete and a preparation method, and relates to the field of building materials, the lightweight
thermal insulation concrete comprises the following components by
mass: 60-100 parts of
cement, 5-10 parts of modified SEBS, 20-40 parts of
fly ash, 30-60 parts of ceramsite, 0.5-1.5 parts of a compound
foaming agent, 10-20 parts of a
modified cellulose filler, 0.005-0.015 part of a foam stabilizer, 0.5-1.5 parts of a
water reducer and 30-50 parts of water; the modified SEBS is prepared from the following raw materials: an SEBS body,
itaconic acid and
allyl glycidyl ether. The preparation method comprises the following steps: mixing and stirring
cement, modified SEBS,
fly ash and
modified cellulose filler, adding ceramsite, and stirring to obtain a dry mixture; preparing a water
reducing agent solution, and preparing a
foaming agent dispersion liquid; adding water into the dry mixture, stirring, adding a water
reducing agent solution, and stirring to obtain a wet mixture; and adding the
foaming agent dispersion liquid into the wet mixture, and carrying out pressure foaming to obtain the lightweight
thermal insulation concrete. The method has the effect of improving the thermal insulation performance and the anti-
cracking performance of the concrete.