[0024] The preparation method of cotton linter fiber of the present invention, it comprises the steps:
[0025] (1) Pulping: material preparation→cooking→bleaching→washing;
[0026] (2) Spinning: viscose pulp → soaking, pressing, dispersing alkali cellulose aging → yellowing → solution mixing → filtration → defoaming → spinning forming.
[0027] In the present invention, the purification yield of described stock preparation is 83-90% of one-course cashmere, 70-80% of two-course cashmere, and the impurity rate of raw material after stock preparation is < 6%.
[0028] In the present invention, the steaming and bleaching are to dissolve and bleach a small amount of impurities remaining on the cotton linters through the method of making cakes; the steaming bleaching agent is hydrogen peroxide.
[0029] In the present invention, the temperature of the cooking and bleaching is 120°C, and the pressure is 4.5kg / cm 2 , the time is 160-180min.
[0030] In the present invention, the w...
Embodiment 1
[0035] Process steps:
[0036] (1) Pulping: material preparation→cooking→bleaching→washing;
[0037] (2) Spinning: viscose pulp → soaking, pressing, dispersing alkali cellulose aging → yellowing → solution mixing → filtration → defoaming → spinning forming.
[0038] The purification yield of described stock preparation is 83% of one velvet, 70% of two velvet, and the impurity rate of raw materials after stock preparation < 6%.
[0039] The cooking and bleaching is to use the method of making cakes to dissolve and bleach a small amount of impurities remaining on the cotton linters through the bleaching agent; the bleaching agent is hydrogen peroxide.
[0040] The temperature of the cooking and bleaching is 120°C, and the pressure is 4.5kg / cm 2 , the time is 160min.
[0041] The washing time is 30 min, and the amount of clean water is 30m 3 / ton pulp.
[0042] Said spinning is dissolving cotton linters pulp in NMMO solvent, after impurity removal and filtration, spinning b...
Embodiment 2
[0046] Process steps:
[0047] (1) Pulping: material preparation→cooking→bleaching→washing;
[0048] (2) Spinning: viscose pulp → soaking, pressing, dispersing alkali cellulose aging → yellowing → solution mixing → filtration → defoaming → spinning forming.
[0049] The purification yield of described stock preparation is 90% of one velvet, 80% of second velvet, and the impurity rate of raw materials after stock preparation < 6%.
[0050] The cooking and bleaching is to use the method of making cakes to dissolve and bleach a small amount of impurities remaining on the cotton linters through the bleaching agent; the bleaching agent is hydrogen peroxide.
[0051] The temperature of the cooking and bleaching is 120°C, and the pressure is 4.5kg / cm 2 , the time is 180min.
[0052] The washing time is 30 min, and the amount of clean water is 30m 3 / ton pulp.
[0053] Said spinning is dissolving cotton linters pulp in NMMO solvent, after impurity removal and filtration, spinnin...
PUM
Property | Measurement | Unit |
---|---|---|
Powerful | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology