Embodiment 1
[0032] The present embodiment provides an antibacterial powder coating for a washing machine, which contains the following components in parts by mass:
[0033] 40 parts epoxy resin
[0034] Polyisocyanate 25 parts
[0035] Glycidyl cyanate 20 parts
[0036] Attapulgite 15 parts
[0037] 7 parts perlite
[0038] Titanium dioxide 26 parts
[0039] 6 parts butyl cellulose
[0040] Organosiloxane 0.7 parts
[0041] Pentaerythritol 1.5 parts
[0042] Antibacterial agent 3 parts.
[0043] The preparation steps of antibacterial powder coating for washing machine are as follows:
[0044] Step 1: Fully mix attapulgite, perlite, titanium dioxide, butyl cellulose, organosiloxane, pentaerythritol and antibacterial agent in the mixture;
[0045] The second step: Add epoxy resin, polyisocyanate and glycidyl cyanate to the mixture, mix well, extrude with twin-screw extruder, crush with claw crusher, pass through 457.2 mesh number / cm (180 mesh) sieve to get the antibacterial powder...
Embodiment 2
[0048] The present embodiment provides an antibacterial powder coating for a washing machine, which contains the following components in parts by mass:
[0049] 35 parts epoxy resin
[0050] Polyisocyanate 23 parts
[0051] Glycidyl cyanate 18 parts
[0052] Attapulgite 14 parts
[0053] 6.5 parts perlite
[0054] Titanium dioxide 22 parts
[0055] Butylcellulose 5 parts
[0056] Organosiloxane 0.6 parts
[0057]Pentaerythritol 1.4 parts
[0058] Antibacterial agent 2.5 parts.
[0059] The preparation steps of antibacterial powder coating for washing machine are as follows:
[0060] Step 1: Fully mix attapulgite, perlite, titanium dioxide, butyl cellulose, organosiloxane, pentaerythritol and antibacterial agent in the mixture;
[0061] The second step: Add epoxy resin, polyisocyanate and glycidyl cyanate to the mixture, mix well, extrude with twin-screw extruder, crush with claw crusher, pass through 457.2 mesh number / cm (180 mesh) sieve to get the antibacterial powd...
Embodiment 3
[0064] The present embodiment provides an antibacterial powder coating for a washing machine, which contains the following components in parts by mass:
[0065] 25 parts epoxy resin
[0066] Polyisocyanate 18 parts
[0067] Glycidyl cyanate 13 parts
[0068] Attapulgite 9 parts
[0069] 4 parts perlite
[0070] Titanium dioxide 15 parts
[0071] Butyl cellulose 3.5 parts
[0072] Organosiloxane 0.45 parts
[0073] 1 part pentaerythritol
[0074] 1.7 parts of antibacterial agent.
[0075] The preparation steps of antibacterial powder coating for washing machine are as follows:
[0076] Step 1: Fully mix attapulgite, perlite, titanium dioxide, butyl cellulose, organosiloxane, pentaerythritol and antibacterial agent in the mixture;
[0077] The second step: Add epoxy resin, polyisocyanate and glycidyl cyanate to the mixture, mix well, extrude with twin-screw extruder, crush with claw crusher, pass through 457.2 mesh number / cm (180 mesh) sieve to get the antibacterial po...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com