A technology of asphalt mixture and asphalt, which is applied in the field of road construction, can solve problems such as threats to human health and the natural environment, high rolling temperature, etc., and achieve the effects of reducing harmful gases, reducing emissions, and reducing energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] This embodiment provides a kind of asphalt mixture, it comprises:
[0021] Asphalt, surfactants, aggregates, mineral powder; the surfactant is a surfactant with a pH value of 9.5±1, an amine value of 400-500mg / g, and a solid content of ≥9.5%.
[0022] The rolling temperature required for the above-mentioned asphalt mixture is 90-130°C. Under this temperature condition, the harmful gas emitted by the asphalt mixture is greatly reduced. The temperature is lowered by at least 20°C, thus reducing the energy consumption for heating during rolling. It can be seen that the above-mentioned asphalt mixture not only reduces the emission of harmful gases during rolling, but also reduces energy consumption, so it is more environmentally friendly and safe to use for asphalt pavement maintenance.
[0023] The reason for the low rolling temperature of the above-mentioned asphalt mixture is that: add a mixture with a pH value of 9.5±1, an amine value of 400-500 mg / g, and a solid conte...
Embodiment 2
[0029] This embodiment provides the preparation method of the asphalt mixture of embodiment one, comprises the following steps:
[0030] Step 101: mixing mineral powder and aggregate and heating to 145-160°C;
[0031] Step 102: heating the asphalt to 145-160°C;
[0032] Step 103: adding a surfactant to the heated asphalt, and stirring to mix;
[0033] Step 104: Mix the mixed asphalt and surfactant with the mixed and heated mineral powder and aggregate, and stir, and control the temperature of the mixture at 135-150° C. during the stirring process.
Embodiment 3
[0035] This embodiment provides a kind of asphalt mixture, it comprises:
[0036] Asphalt, surfactant, aggregate, mineral powder and polyester fiber; the surfactant is a surfactant with a pH value of 9.5±1, an amine value of 400-500mg / g, and a solid content of ≥9.5%.
[0037] Compared with Example 1, the Marshall stability of the asphalt mixture in this embodiment is higher and the work performance is better, because: the polyester fiber in the asphalt mixture plays the role of adsorption, absorbing asphalt and improving the cohesion of the asphalt mixture It also has the function of dispersing asphalt mineral powder and stabilizing asphalt film.
[0038] In addition, the asphalt used in all the above examples may preferably use high-strength asphalt or styrene-butadiene-styrene block copolymer (SBS) modified asphalt.
[0039] The high-strength asphalt mentioned above refers to asphalt with the following technical indicators:
[0040] The penetration of a load of 100 grams i...
PUM
Property | Measurement | Unit |
---|---|---|
penetration | aaaaa | aaaaa |
flash point | aaaaa | aaaaa |
softening point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com