Method for removing feldspar in quartz sand through flotation
A quartz sand and flotation technology, applied in flotation, solid separation and other directions, can solve the problem of unsatisfactory feldspar removal effect, and achieve the effects of convenient operation, reduced labor intensity and reduced production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A method for removing feldspar by quartz sand flotation, comprising the following steps:
[0019] (1) Crushing: Crushing the raw material quartz ore to 0.1-1μm, adding water, mixing and stirring to prepare pulp A;
[0020] (2) pH adjustment: add alkaline substances to the pulp A to obtain pulp B with pH=11~12, the alkaline substance is one or more combinations of caustic soda, soda ash and ammonia water ;
[0021] (3) Adding activator, collector and 1-dodecanol to the pulp B, and stirring evenly to obtain pulp C;
[0022] (4) Put the pulp C into a flotation machine for flotation to obtain quartz sand from which feldspar has been removed.
Embodiment 2
[0024] A method for removing feldspar by quartz sand flotation, comprising the following steps:
[0025] (1) Crushing: Crushing the raw material quartz ore to 0.1-1μm, adding water, mixing and stirring to prepare pulp A;
[0026] (2) pH adjustment: add alkaline substances to the pulp A to obtain pulp B with pH=11~12, the alkaline substance is one or more combinations of caustic soda, soda ash and ammonia water ;
[0027] (3) Add an activator, a collector and 1-dodecanol to the pulp B, and stir evenly to obtain a pulp C; the activator is a compound that can be hydrolyzed into magnesium ions;
[0028] (4) Put the pulp C into a flotation machine for flotation to obtain quartz sand from which feldspar has been removed.
[0029] Preferably, the collector in step (3) is an alkyl sulfonate.
Embodiment 3
[0031] A method for removing feldspar by quartz sand flotation, comprising the following steps:
[0032] (1) Crushing: Crushing the raw material quartz ore to 0.1-1μm, adding water, mixing and stirring to prepare pulp A;
[0033] (2) pH adjustment: add alkaline substances to the pulp A to obtain pulp B with pH=11~12, the alkaline substance is one or more combinations of caustic soda, soda ash and ammonia water , the addition of alkaline substances is to adjust the pH of pulp B=11~12;
[0034] (3) Add an activator, a collector and 1-dodecanol to the pulp B, and stir evenly to obtain a pulp C; the activator is a compound that can be hydrolyzed into magnesium ions; the The collector is alkyl sulfonate; the addition amount of activator, collector and 1-dodecanol is 0.01~0.05% of the mass of pulp B;
[0035] (4) Put the pulp C into a flotation machine for flotation to obtain quartz sand from which feldspar has been removed.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com